The rare earths (RE) are characterized with their strong metallic atomic bonds. They are used in magnetic materials used in computer technology and electric powered vehicles. The advancing globalization and the increasing standard of living both lead to massive waste disposal problems, therefore, the methods of recovering used metallic materials are sought. In this paper, the microscopic characteristic of magnetic powder from old electric engines has been presented.
Czasopismo
Rocznik
Tom
Strony
39--41
Opis fizyczny
Bibliogr. 8 poz., rys.
Twórcy
autor
- University of Technology, Clausthal Centre of Material Technology, Agricolastraße 6, 38678 Clausthal-Zellerfeld, Germany, EU, German Federal Environmental Foundation
autor
- Institute of Polymer and Plastics Engineering, Agricolastraße 6, 38678 Clausthal-Zellerfeld, Germany, EU
autor
- University of Technology, Clausthal Centre of Material Technology, Agricolastraße 6, 38678 Clausthal-Zellerfeld, Germany, EU
autor
- University of Technology, Department of Mineral and Waste Processing, Walther-Nerst-Strasse 9, 38678 Clausthal-Zellerfeld, Germany, EU
autor
- Czestochowa University of Technology, Department of Production Engineering and Safety, ul. Armii Krajowej 19 B 42-200 Czestochowa, Poland, EU
Bibliografia
- [1] Callister, William D. (2002) Materials Science and Engineering an Introduction, New York, Hoffman Press, pp. 673-700. Vol. 11.
- [2] Cohen, Morris, [ed.] (1972), Introduction to Magnetic Materials, Reasing Massachusetts, Addison-Wesley Publishing Company, pp. 181-202, 287-351, 556-626, Vol.11.
- [3] Weng, Robert S., WIJ, Jiin-Chuan and Kryder, Mark H. (1991) The effect of random coercivity on domain growth processes in rare earth-transition metal alloys, Vol. 69,8, pp. 4856-4856.
- [4] Klimecka-Tatar D., Bala H., Ślusarek B., Jagielska-Wiaderek K. (2009) The Effect of Consolidation Method on Electrochemical Corrosion of Polymer Bonded Nd-Fe-B Type Magnetic Material. Arch Metall Mater 54/1, s. 247-256.
- [5] Elwert, T., & Goldmann, D. (2015) Entwicklung eines hydrometallurgischen Recyclingverfahrens für NdFeB-Magnete. Universitätsbibliothek Clausthal.
- [6] Berkowitz, Ami E. and Kneller, Eckart (1969) Magnetism and Metallurgy, New York, Academic Press, Inc.
- [7] Zakotnik, M., Harris, I. R., & Williams (2008) A. J. Possible methods of recycling NdFeB-type sintered magnets using the HD/degassing process. Journal of Alloys and Compounds, 450(1), 525-531.
- [8] Wnuk I., Wyslocki J. and Pryzbyl A. (2007) Phase struckture of nanocrystalline Nd2Fe14B magnets with different grain size, pp. 85-88.
Uwagi
Opracowanie ze środków MNiSW w ramach umowy 812/P-DUN/2016 na działalność upowszechniającą naukę (zadania 2017).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-aa1b8cb3-636c-4c8e-b58c-74eb6272dc0a