Alumina/graphene composite in friction and wear tests at elevated temperatures

Wybrane pełne teksty z tego czasopisma
Identyfikatory
Warianty tytułu
PL
Kompozyt tlenek glinu/grafen w testach tarcia i zużycia w podwyższonych temperaturach
Języki publikacji
EN
Abstrakty
EN
Alumina materials are of great interest due to their high wear resistance, resistance to corrosion, high strength and low friction. However, studies show that a graphene addition can significantly reduce wear and friction. Even a small addition of platelets results in noticeable changes in the material properties. The presented work describes the results of the ball-on-disc test conducted on two friction pairs: alumina-alumina and alumina/graphene composite - alumina. The tests were conducted at four temperatures: 20, 150, 300 and 500°C in air. Surface profile geometry measurements after the test were used to determine the wear rate. Observation of the surface microstructure after friction was carried out using a scanning electron microscope. The tests showed improvement in the wear resistance and a decrease in the friction coefficient of the composite tested at room temperature compared to pure alumina, while the use of elevated temperatures adversely affected the composite.
PL
Materiały z tlenku glinu cieszą się dużym zainteresowaniem ze względu na wysoką odporność na zużycie, odporność na korozję, wysoką wytrzymałość i niewielkie tarcie. Badania pokazują jednak, że dodatek grafenu może znacznie zmniejszyć zużycie i tarcie. Nawet niewielki dodatek płytek powoduje zauważalne zmiany właściwości. W pracy przedstawiono wyniki badań w teście Ball-on-Disc przeprowadzonych na dwóch parach ciernych: tlenek glinu-tlenek glinu oraz kompozycie tlenek glinu/grafen- tlenek glinu. Badania przeprowadzono w czterech temperaturach: 20, 150, 300 i 500°C w powietrzu. Pomiary geometrii profili powierzchni po próbach wykorzystano do wyznaczenia wskaźnika zużycia. Obserwację mikrostrukturalną zużytych powierzchni prowadzono za pomocą skaningowego mikroskopu elektronowego. Badania wykazały poprawę odporności na zużycie i zmniejszenie współczynnika tarcia kompozytu badanego w temperaturze pokojowej w porównaniu z czystym tlenkiem glinu, natomiast zastosowanie podwyższonych temperatur miało negatywny wpływ na kompozyt.
Rocznik
Strony
162--166
Opis fizyczny
Bibliogr. 10 poz., rys., tab.
Twórcy
autor
  • AGH - University of Science and Technology, Faculty of Materials Science and Ceramics, Department of Ceramics and Refractory Materials, al. Mickiewicza 30, 30-059 Krakow, Poland
autor
  • AGH - University of Science and Technology, Faculty of Mechanical Engineering and Robotics, Department of Machine Design and Technology, al. Mickiewicza 30, 30-059 Krakow, Poland
autor
  • AGH - University of Science and Technology, Faculty of Materials Science and Ceramics, Department of Ceramics and Refractory Materials, al. Mickiewicza 30, 30-059 Krakow, Poland
autor
  • AGH - University of Science and Technology, Faculty of Materials Science and Ceramics, Department of Ceramics and Refractory Materials, al. Mickiewicza 30, 30-059 Krakow, Poland
autor
  • AGH - University of Science and Technology, Faculty of Materials Science and Ceramics, Department of Ceramics and Refractory Materials, al. Mickiewicza 30, 30-059 Krakow, Poland
autor
  • AGH - University of Science and Technology, Faculty of Materials Science and Ceramics, Department of Ceramics and Refractory Materials, al. Mickiewicza 30, 30-059 Krakow, Poland
autor
  • AGH - University of Science and Technology, Faculty of Materials Science and Ceramics, Department of Ceramics and Refractory Materials, al. Mickiewicza 30, 30-059 Krakow, Poland
autor
  • AGH - University of Science and Technology, Faculty of Mechanical Engineering and Robotics, Department of Machine Design and Technology, al. Mickiewicza 30, 30-059 Krakow, Poland
autor
  • AGH - University of Science and Technology, Faculty of Materials Science and Ceramics, Department of Ceramics and Refractory Materials, al. Mickiewicza 30, 30-059 Krakow, Poland
Bibliografia
  • [1] Zeng P., Rainforth W.M., Stewart T.D., Characterisation of the wear mechanisms in retrieved alumina-on-alumina total hip replacements, Wear 2017, 376-377, 212-222.
  • [2] Manojkumar P.A., Gandhi A.S., Kamaraj M., Tyagi A.K., Sliding wear behaviour of alumina coatings prepared from mechanically milled powders, Wear 2014, 313, 1-2, 11-18.
  • [3] Xiong F., Manory R.R., The effect of test parameters on alumina wear under low contact stress, Wear 1999, 236, 240-245.
  • [4] Gutierrez-Gonzalez C.F., Smirnov A., Centeno A., Fernández A., Alonso B., Rochad V.G., Torrecillas R., Zurutuza A., Bartolome J.F., Wear behavior of graphene/alumina composite, Ceramics International 2015, 41, 7434-7438.
  • [5] Rutkowski P., Klimczyk P., Jaworska L., Stobierski L., Zientara D., Tran K., Mechanical properties of pressure sintered alumina-graphene composites, Materiały Ceramiczne/Ceramic Materials 2016, 68, 2, 168-175.
  • [6] Ahmad I., Kennedy A., Zhu Q.Y., Wear resistant properties of multiwalled carbon nanotubes reinforced Al2O3 nanocomposites, Wear 2010, 269, 71-78.
  • [7] Markandan K., Chin J.K., Tan M.T.T., Recent progress in graphene based ceramic composites: a review, International Journal of Materials Research 2017, 32, 84-106.
  • [8] Gutiérrez-Mora F., Cano-Crespo R., Rincón A., Moreno R., Domínguez-Rodríguez A., Friction and wear behavior of alumina-based graphene and CNFs composites, Journal of the European Ceramic Society 2017, 37, 3805-3812.
  • [9] Wojteczko A., Wiązania G., Kot M., Pędzich Z., Friction and wear of composites in alumina/zirconia system, Composites Theory and Practice 2018, 18, 1, 51-56.
  • [10] ISO 20808:2016 Standard, Determination of friction and wear characteristics of monolithic ceramics by ball-on-disc method.
Uwagi
Opracowanie rekordu w ramach umowy 509/P-DUN/2018 ze środków MNiSW przeznaczonych na działalność upowszechniającą naukę (2018).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-9cec59ef-df17-430d-a74c-3c1d71717551
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.