Brazing of Alloy Based on Fe3Al Aluminide

Treść / Zawartość
Identyfikatory
Warianty tytułu
PL
Lutowanie twarde stopu na osnowie aluminidku Fe3Al
Języki publikacji
EN
Abstrakty
EN
Alloys based on the Fe3Al intermetallic phase belong to a new generation of metallic materials intended for operation at higher temperatures and having properties something between those of metals and ceramic materials. They are characterised by relatively high oxidation resistance, high corrosion resistance, high-temperature creep resistance, high electrical resistivity, high abrasion resistance as well as resistance to erosion and cavitation. Although the material costs of these alloys are relatively low, they belong to materials which are very difficult to join by means of welding methods. For this reason, joining such materials remains an important and current research and technological problem. One of the methods used for joining such materials is brazing. This work shows the results of technological tests concerned with vacuum brazing an alloy based on the Fe3Al (Fe86Al14) phase using silver (Ag72Cu28) and copper-nickel (Cu90Ni210, Cu95Ni5) filler metals as well as presents the results of tests on the mechanical and structural properties of obtained joints.
PL
Stopy na osnowie fazy międzymetalicznej typu Fe3Al należą do nowszej generacji materiałów metalicznych, przeznaczonych do pracy w podwyższonych temperaturach, o właściwościach pośrednich pomiędzy metalami a materiałami ceramicznymi. Charakteryzują się one przede wszystkim stosunkowo wysoką odpornością na utlenianie i korozje, żarowytrzymałością, wysoką rezystywnością elektryczną, a także wysoką odpornością na ścieranie, erozje i kawitacje. Stopy te, o stosunkowo niskich kosztach materiałowych, należą jednak do materiałów bardzo trudno spajalnych metodami spawalniczymi, dlatego zagadnienie ich łączenia stanowi wciąż ważny i aktualny problem badawczy oraz technologiczny. Jedna z metod łączenia takich materiałów jest lutowanie twarde. W niniejszej pracy przedstawiono wyniki badań technologicznych z zakresu lutowania próżniowego stopu na osnowie fazy Fe3Al (Fe86Al14), spoiwami: srebrnym (Ag72Cu28) i miedziano-niklowymi (Cu90Ni210, Cu95Ni5), a także wyniki badań właściwości wytrzymałościowych i strukturalnych uzyskanych połączeń.
Twórcy
autor
  • Department of Welding Technology in Instytut Spawalnictwa (Institute of Welding) – Gliwice, Poland
  • Department of Welding Technology in Instytut Spawalnictwa (Institute of Welding) – Gliwice, Poland
Bibliografia
  • [1] Z. Bojara, W. Przetakiewicz, Materiały metalowe z udziałem faz międzymetalicznych. BEL Studio, Warszawa (2006) (in Polish).
  • [2] R. W. Messler, Joining of Advanced Materials. Butterworth - Heineman, Stoneham (1993).
  • [3] S. C. Deevi, V. K. Sikka, C. T. Liu, Progress in Materials Science 42, 177-192(1997).
  • [4] J. Adamiec, P. Adamiec, Kongres JOIN-TEC 189 (2003).
  • [5] J. Adamiec, A. Grabowski, A. Lisiecki, Materiały konferencyjne, 7STL,Szczecin (2002) (in Polish).
  • [6] J. Adamiec, P. Adamiec, M. Więcek, Acta Metallurgica Slovaca 10, 745-748 (2004).
  • [7] W. Włosiński, T. Chmielewski, M. Kucharczyk, Przegląd Spawalnictwa 1, 222-228, 2004 (in Polish).
  • [8] Z. Li, R. K. Shiue, S. K. Wu, Intermetallics 18, 422-428 ( 2010).
  • [9] R. K. Shiue, S. K. Wu, Lee Y. L., Intermetallics 13, 818-826 (2005).
  • [10] R. K. Shiue, S. K. Wu, I-H Lee, Gold Bull 44, 49-56 (2011).
  • [11] Y. L. Lee, R. K. Shiue, S. K. Wu, Intermetallics 11, 187-195 (2003).
  • [12] A. Winiowski, M. Różański, Kovove Materialy 51, 2, 123 -128 (2013).
  • [13] Z. Mirski, M. Różanski, Archives of Civil and Mechanical Engineering, 13 no 4, 415-421, (2013).
  • [14] A. Winiowski, Archives of Metallurgy and Materials, 55, 4, 991-1000, (2010).
  • [15] W. Gąsior, A. Winiowski, Archives of Metallurgy and Materials 57, 4, 1087-1093 , (2012).
  • [16] A. Winiowski, M. Różański, Archives of Metallurgy and Materials 58, 4, 1007-1011 (2013).
  • [17] A. Winiowski, M. Różański, Welding International 5, 331-335 (2011).
  • [18] A. Winiowski, M. Różański, The Final Report of Statutory R&D Activity. Cc-53, Instytut Spawalnictwa, Gliwice (2010) (in Polish).
  • [19] PN-EN ISO 17672:2010, Brazing - Filler metals.
  • [20] PN-EN 12797:2002, Brazing -Destructive tests of brazed joints.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-9b98049d-1437-4dce-89d9-37c21349bb03
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.