he scientific and industrial communities now consider surface modification of steel-based alloys to be essential. One effective method of altering these alloys' surfaces is tungsten inert gas (TIG) cladding.The purpose of this study is to investigate how the surface characteristics of austenitic stainless steel substrates are affected by TIG-deposited composite coatings made of tungsten carbide and nickel (WC-Ni). The study also intends to investigate the influence of the WC-Ni composite coatings' travel speed, and as a result, the heat input usually has significant effects on the microstructure. The coating layers were deposited at different travel speeds (67, 107, and 122 mm/min) using pre-placed composite pastes that were 1 mm thick and contained the same weight percentage of WC (65). The clad layers showed a variety of microstructures in optical and scanning electron microscopy, primarily nickel solid solution dendrites with WC particles scattered throughout the matrix. The dendrites at various locations across the clad layers were few or dense, finer or coarser, equiaxial or columnar, densely or less densely branched, depending on the cooling rates and the density of WC in the composite. Energy dispersive spectroscopy demonstrated that the Fe element that was transferred from the substrate material to the molten pool was primarily concentrated in the matrix, not the dendrites, while the dendrite locations and orientations were amply demonstrated by the distribution of the W element.
Twórcy
  • Faculty of Materials Engineering, University of Babylon, Hillah, Babil, Iraq
  • Faculty of Materials Engineering, University of Babylon, Hillah, Babil, Iraq
Bibliografia
  • 1. Lo K.H., Shek C.H., Lai J.K. Recent developments in stainless steels. Materials Science and Engineering: R: Reports. 2009, 65(4–6): 39–104.
  • 2. Baddoo N.R. Stainless steel in construction: A review of research, applications, challenges and opportunities. Journal of constructional steel research. 2008, 64(11): 1199–206.
  • 3. Rossi B. Discussion on the use of stainless steel in constructions in view of sustainability. Thin-Walled Structures. 2014, 83: 182–9.
  • 4. Davis J.R. editor. Stainless steels. ASM international; 1994.
  • 5. Rius-Ayra O., Llorca-Isern N. Surface modification of metals and alloys. Coatings. 2021, 11(2): 260.
  • 6. Bose S., Robertson S.F., Bandyopadhyay A. Surface modification of biomaterials and biomedical devices using additive manufacturing. Acta biomaterialia. 2018, 66: 6–22.
  • 7. Khan A. Tungsten Inert Gas Welding (TIG) Principles,6 Parts, Applications, Pros, Cons. Dizz. 2018.
  • 8. Kaulgud O.M., Chavan S.T. Process Parameter Optimization of TIG Welding by Taguchi Method and Its Effect on Performance Parameter of Stainless Steel Grade 302HQ. International Transaction Journal of Engineering, Management, & Applied Sciences & Technologies. 2022, 13(7).
  • 9. Singh J., Thakur L., Angra S. Effect of argon flow rate and standoff distance on the microstructure and wear behaviour of WC-CoCr TIG cladding. InJournal of Physics: Conference Series. 2019, 1240(1): 012162. IOP Publishing.
  • 10. Kilic M., Imak A., Kirik I. Surface modification of AISI 304 stainless steel with NiBSi-SiC composite by TIG method. Journal of Materials Engineering and Performance. 2021, 30(2): 1411–9.
  • 11. Kumar S., Ghosh P.K. Thermal behaviour of TIG arc surfacing affecting mechanical properties of AISI 4340 steel substrate under static and dynamic loading. Materials Science and Engineering: A. 2020, 773: 138734.
  • 12. Davis J.R., editor. Surface hardening of steels: understanding the basics. ASM international; 2002.
  • 13. Karmakar R., Maji P., Ghosh S.K. A review on the nickel based metal matrix composite coating. Metals and Materials International. 2021, 27: 2134–45.
  • 14. Ashebir D.A., Mengesha G.A., Sinha D.K. An insight into mechanical and metallurgical behavior of hybrid reinforced aluminum metal matrix composite. Advances in Materials Science and Engineering. 2022.
  • 15. Chawla, K.K., Chawla, K.K. Metal matrix composites. Springer New York. 1998, 164–211.
  • 16. Yan H., Zhang P., Yu Z., Lu Q., Yang S., Li C. Microstructure and tribological properties of laser-clad Ni–Cr/TiB2 composite coatings on copper with the addition of CaF2. Surface and Coatings Technology. 2012, 206(19–20): 4046–53.
  • 17. Karthik B.M., Gowrishankar M.C., Sharma S.S., Hiremath P., Shettar M., Shetty N. Coated and uncoated reinforcements metal matrix composites characteristics and applications–A critical review. Cogent Engineering. 2020, 7(1): 1856758.
  • 18. Liu K., editor. Tungsten carbide: processing and applications. BoD–Books on Demand; 2012 Dec 19.
  • 19. Grairia A., Beliardouh N.E., Zahzouh M., Nouveau C., Besnard A. Dry sliding wear investigation on tungsten carbide particles reinforced iron matrix composites. Materials Research Express. 2018, 5(11): 116528.
  • 20. Lisiecki A., Ślizak D. Hybrid laser deposition of composite WC-Ni layers with forced local cryogenic cooling. Materials. 2021, 14(15): 4312.
  • 21. Farahmand P., Kovacevic R. Parametric study and multi-criteria optimization in laser cladding by a high power direct diode laser. Lasers in Manufacturing and Materials Processing. 2014, 1: 1–20.
  • 22. Jeyaprakash N., Yang C.H., Kumar D.R. Laser surface modification of materials. Practical Applications of Laser Ablation. 2020, 61–81.
  • 23. Hong C., Gu D., Dai D., Cao S., Alkhayat M., Jia Q., Gasser A., Weisheit A., Kelbassa I., Zhong M., Poprawe R. High-temperature oxidation performance and its mechanism of TiC/Inconel 625 composites prepared by laser metal deposition additive manufacturing. Journal of laser applications. 2015, 27(1).
  • 24. Kumar V., Lucas B., Howse D., Melton G., Raghunathan S., Vilarinho L. Investigation of the A-TIG Mechanism and the Productivity Benefits in TIG Welding. In15th International Conference on the Joining of Materials (JOM 15) and 6th International Conference on Education in Welding (ICEW 6) Helsingor, Denmark 2009, 3–6.
  • 25. Prasad R., Waghmare D.T., Kumar K., Masanta M. Effect of overlapping condition on large area NiTi layer deposited on Ti-6Al-4V alloy by TIG cladding technique. Surface and Coatings Technology. 2020, 385: 125417.
  • 26. Lailatul P.H., Maleque M.A. Surface modification of duplex stainless steel with SiC preplacement using TIG torch cladding. Procedia engineering. 2017, 184: 737–42.
  • 27. Ghadami F., Sohi M.H., Ghadami S. Effect of TIG surface melting on structure and wear properties of air plasma-sprayed WC–Co coatings. Surface and Coatings Technology. 2015, 261: 108–13.
  • 28. Haldar B., Saha P. Identifying defects and problems in laser cladding and suggestions of some remedies for the same. Materials Today: Proceedings. 2018, 5(5): 13090–101.
  • 29. Van Acker K., Vanhoyweghen D., Persoons R., Vangrunderbeek J. Influence of tungsten carbide particle size and distribution on the wear resistance of laser clad WC/Ni coatings. wear. 2005, 258(1–4): 194–202.
  • 30. Singh J., Thakur L., Angra S. Abrasive wear behavior of WC-10Co-4Cr cladding deposited by TIG welding process. International Journal of Refractory Metals and Hard Materials. 2020, 88: 105198.
  • 31. Buytoz S., Ulutan M., Yildirim M.M. Dry sliding wear behavior of TIG welding clad WC composite coatings. 32. Tosun G. Ni–WC coating on AISI 1010 steel using TIG: microstructure and microhardness. Arabian Journal for Science and Engineering. 2014, 39: 2097–106.
  • 32. Tosun G. Ni–WC coating on AISI 1010 steel using TIG: microstructure and microhardness. Arabian Journal for Science and Engineering. 2014, 39: 2097–106.
  • 33. Lin Y.C., Chang K.Y. Elucidating the microstructure and wear behavior of tungsten carbide multi-pass cladding on AISI 1050 steel. Journal of Materials Processing Technology. 2010, 210(2): 219–25.
  • 34. Dai Q.L., Luo C.B., You F.Y. Crack restraining methods and their effects on the microstructures and properties of laser cladded WC/Fe coatings. Materials. 2018, 11(12): 2541.
  • 35. Ma Q., Li Y., Wang J., Liu K. Investigation on coredeutectic structure in Ni60/WC composite coatings fabricated by wide-band laser cladding. Journal of Alloys and Compounds. 2015, 645: 151–7.
  • 36. Yazdi R., Kashani-Bozorg S.F. Microstructure and wear of in-situ Ti/(TiN+ TiB) hybrid composite layers produced using liquid phase process. Materials chemistry and physics. 2015, 152: 147–57.
  • 37. Nowotny S., Berger L.M., Spatzier J. Coatings by laser cladding.
  • 38. Pawlowski L. Thick laser coatings: A review. Journal of Thermal Spray Technology. 1999, 8: 279–95.
  • 39. Liu Y.H., Li J., Xuan F.Z. Fabrication of TiC reinforced Ni based coating by laser cladding. Surface Engineering. 2012, 28(8), 560–3.
  • 40. Cui C., Guo Z., Wang H., Hu J. In situ TiC particles reinforced grey cast iron composite fabricated by laser cladding of Ni–Ti–C system. Journal of Materials Processing Technology. 2007, 183(2–3): 380–5.
  • 41. Li Y., Bai P., Wang Y., Hu J., Guo Z. Effect of TiC content on Ni/TiC composites by direct laser fabrication. Materials & Design. 2009, 30(4), 1409–12.
  • 42. Shravan C., Radhika N., Deepak Kumar N.H., Sivasailam B. A review on welding techniques: properties, characterisations and engineering applications. Advances in Materialsand Processing Technologies. 2023, 10: 80.
  • 43. Padilha A.F., Rios P.R. Decomposition of austenite in austenitic stainless steels. ISIJ international. 2002, 42(4): 325–7.
  • 44. Karaman I., Sehitoglu H., Maier H.J., Chumlyakov Y.I. Competing mechanisms and modeling of deformation in austenitic stainless steel single crystals with and without nitrogen. Acta Materialia. 2010, 49(19): 3919–33.
  • 45. Gavriljuk V.G. and Berns H. High Nitrogen Steels. Springer-Verlag, Berlin. 1999.
  • 46. Chumlyakov Y.I., Kireeva I.V., Korotaev A.D. Plastic deformation of single crystals of austenitic stainless steels strengthened by nitrogen. I: Orientation and temperature dependence of critical shear stress. Physics of Metals and Metallography. 1992, 73(4): 429–34.
  • 47. Chumlyakov Y.I., Kireeva I.V. and Ivanova O.V. Phys. Met. Metall. 1994, 78: 350.
  • 48. Hull D. and Bacon D.J. Dislocations. Oxford University Press, New York, 1989.
  • 49. Evangeline A, Sathiya P. Structure–property relationships of Inconel 625 cladding on AISI 316L substrate produced by hot wire (HW) TIG metal deposition technique. Materials Research Express. 2019, 6(10): 106539.
  • 50. Hassan K.A., Prangnell P.B., Norman A.F., Price D.A., Williams S.W. Effect of welding parameters on nugget zone microstructure and properties in high strength aluminium alloy friction stir welds. Science and Technology of Welding and joining. 2003, 8(4): 257–68.
Uwagi
Opracowanie rekordu ze środków MNiSW, umowa nr SONP/SP/546092/2022 w ramach programu "Społeczna odpowiedzialność nauki" - moduł: Popularyzacja nauki i promocja sportu (2024).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-97c334fb-c428-426b-b948-8afc84c0f458
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.