The Analysis of Filler Material Effect on Properties of Excavator Crawler Track Shoe after Welding Regeneration

Treść / Zawartość
Identyfikatory
Warianty tytułu
Języki publikacji
EN
Abstrakty
EN
The application of hardfacing is one of the ways to restore the functional properties of worn elements. The possibility of using filler materials rich in chrome allows for better wear resistance than base materials used so far. The paper presents the results of research on the use of 3 different grades of covered electrodes for the regeneration of worn track staves. The content of the carbon in the covered electrodes was from 0,5% to 7% and the chromium from 5% to 33%. The microscopic and hardness tests revealed large differences in the structure and properties of the welds. The differences in the hardness of the welds between the materials used were up to 150 HV units. The difference in wear resistance, in the ASTM G65 test, between the best and worst materials was almost 12 times big.
Słowa kluczowe
Twórcy
autor
  • Czestochowa University of Technology, Faculty of Mechanical Engineering and Computer Science, Dąbrowskiego 69, 42-201 Częstochowa, Poland
autor
  • Czestochowa University of Technology, Faculty of Mechanical Engineering and Computer Science, Dąbrowskiego 69, 42-201 Częstochowa, Poland
autor
  • Czestochowa University of Technology, Faculty of Production Engineering and Materials Technology, Dąbrowskiego 69, 42-201 Częstochowa, Poland
autor
  • University of Žilina, Department of Technological Engineering, Univerzitná 1, 010 26 Žilina, Slovakia
autor
  • University of Žilina, Department of Technological Engineering, Univerzitná 1, 010 26 Žilina, Slovakia
Bibliografia
  • [1] J. Tomków, D. Fydrych, G. Rogalski, Materials 12 (20), 3372 (2019), DOI:10.3390/ma12203372.
  • [2] J. Tomków, A. Czupryński, D. Fydrych, Coatings 10, 219 (2020) DOI:10.3390/coatings10030219.
  • [3] A. Zikin, I. Hussainova, C. Katsich, E. Badisch, C. Tomastik, Surf. Coat. Technol. 206, 4270-4278 (2012), DOI:10.1016/j.surfcoat.2012.04.039.
  • [4] M. Kirchgaßner, E. Badisch, F. Franek, Wear. 265, 772-779 (2008), DOI:10.1016/j.wear.2008.01.004.
  • [5] C.M. Lin, H.H. Lai, J.C. Kuo, W. Wu, Mater. Charact. 62, 1124-1133 (2011), DOI:10.1016/j.matchar.2011.09.007.
  • [6] X.H. Wang, F. Han, X.M. Liu, S.Y. Qu, Z.D. Zou, Mater. Sci. Eng. A. 489, 193-200 (2008), DOI:10.1016/j.msea.2007.12.020.
  • [7] M. Szala, L. Łatka, M. Walczak, M. Winnicki, Metals 10 (7), 856 (2020), DOI:10.3390/met10070856.
  • [8] T. Chmielewski, P. Siwek, M. Chmielewski, A. Piątkowska, A. Grabias, D. Golański, Metals 8 (12), 1059 (2018), DOI:10.3390/met8121.
  • [9] M. Adamiak, A. Czupryński, A. Kopyść, Z. Monica, M. Olender, A. Gwiazda, Metals 8, 142 (2018), DOI:10.3390/met8020142.
  • [10] A. Czupryński, J. Górka, M. Adamiak, B. Tomiczek, Arch. Metall. Mater. 61, 1363-1370 (2016), DOI:10.1515/amm-2016-0224.
  • [11] J. Górka, A. Czupryński, M. Żuk, M. Adamiak, A. Kopyść, Materials 11, 1184 (2018), DOI:10.3390/ma11071184.
  • [12] J. Górka, J. Min. Metall. Sect. B-Metall. DOI:10.2298/accepted_manuscript (pdf).
  • [13] V. Jankauskas, M. Antonov, V. Varnauskas, Re. Skirkus, D. Goljandin, Wear. 328-329, 378-390 (2015), DOI:10.1016/j.wear.2015.02.063.
  • [14] D.J. Kotecki, J.S. Ogborn, Weld. J. 74 (8), 269-278 (1995).
  • [15] J.J. Coronado, Wear. 270, 287-293 (2011), DOI:10.1016/j.wear.2010.10.070.
  • [16] H.H. Lai, C.C. Hsieh, C.M. Lin, W. Wu, Surf. Coat. Technol. 239, 233-239 (2014), DOI:10.1016/j.surfcoat.2013.11.048.
  • [17] Y. Lv, Y. Sun, J. Zhao, G. Yu, J. Shen, S. Hu, Mater. Des. 39, 303-308 (2012), DOI:10.1016/j.matdes.2012.02.048.
  • [18] S.D. Carpenter, D.E.O.S. Carpenter, J.T.H. Pearcec, J. Alloys Compd. 494, 245-251 (2010), DOI:10.1016/j.jallcom.2009.12.197.
  • [19] S. Liu, Y. Zhou, X. Xing, J. Wang, X. Ren, Q. Yang, Sci. Rep. 32941, 1-8 (2016), DOI:10.1038/srep32941.
  • [20] X. Qi, Z. Jia, Q. Yang, Y. Yang, Surf. Coat. Technol. 205, 5510-5514 (2011), DOI:10.1016/j.surfcoat.2011.06.027.
  • [21] Y.F. Zhou, Y.L. Yang, Y.W. Jiang, J. Yang, X.J. Ren, Q.X. Yang, Mater. Charact. 72, 77-86 (2012), DOI:10.1016/j.matchar.2012.07.004.
  • [22] S. Xing, S. Yu, Y. Deng, M. Dai, L. Yu, Journal of Rare Earths 30, 69-73 (2012), DOI:10.1016/S1002-0721(10)60641-2.
  • [23] J.J. Coronado, H.F. Caicedo, A.L. Gómez, Tribol. Int. 42, 745-749 (2009), doi:10.1016/j.triboint.2008.10.012.
  • [24] M.F. Buchely, J.C. Gutierrez, L.M. León, A. Toro, Wear 259, 52-61 (2005), doi:10.1016/j.wear.2005.03.002.
  • [25] E.O. Correa, N.G. Alcântara, L.C. Valeriano, N.D. Barbedo, R.R. Chaves, Surf. Coat. Technol. 276, 479-484 (2015), DOI:10.1016/j.surfcoat.2015.06.026.
  • [26] N.G. Chaidemenopoulos, P.P. Psyllaki, E. Pavlidou, G. Vourlias, Surf. Coat. Technol. 357, 651-661 (2019), DOI:10.1016/j.surf-coat.2018.10.061.
  • [27] S. Pawara, A.K. Jha, G. Mukhopadhyay, Int. J. Refract. Met. H. 78, 288-295 (2019), DOI:10.1016/j.ijrmhm.2018.10.014.
  • [28] C.M. Chang, C.M. Lin, C.C. Hsieh, J.H. Chen, C.M. Fan, W. Wu, Mater. Chem. Phys. 117, 257-261 (2009), DOI:10.1016/j.matchemphys.2009.05.052.
  • [29] S. Chatterjee, T.K. Pal, Wear 255, 417-425 (2003), DOI:10.1016/S0043-1648(03)00101-7.
  • [30] M. Gucwa, J. Winczek, M. Mician, Weld. Tech. Rev. 92 (2), 7-14 (2020), DOI:10.26628/wtr.v92i2.1096.
  • [31] C.M. Chang, Y.C .Chen, W. Wu, Tribol.Int. 43, 929-934 (2010), DOI:10.1016/j.triboint.2009.12.045.
Uwagi
Opracowanie rekordu ze środków MNiSW, umowa Nr 461252 w ramach programu "Społeczna odpowiedzialność nauki" - moduł: Popularyzacja nauki i promocja sportu (2021).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-8a56a7a2-e678-41c1-9e19-795506adfe2f
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.