Use of Pinched Sluice in Albite Concentration

Treść / Zawartość
Identyfikatory
Warianty tytułu
PL
Wykorzystanie wzbogacalnika poziomo-prądowego do wzbogacania albitu
Języki publikacji
EN
Abstrakty
EN
Albite (NaAlSi3O8) is an important industrial mineral especially for ceramic and glass production. Major Fe-containing impurity of albite ore is flaky mica minerals. This study was conducted to determine the applicability of pinched sluicing for pre-concentration of albite ore by exploiting shape effect. Effects of feed solid rate, tilting angle of pinched sluice, and splitter position on the rejection of Fe-containing flaky mica were tested. Pulp solid rate was determined to be the most important variable on the rate of mica rejection. Increasing the tilting angle adversely affected the separation efficiency especially above 17°. Distribution of gangue mica in the vertical cross-section of flowing film was tested manipulating the splitter height. Mica particles were observed to be crowded in upper layers of film thickness. So, flaky mica impurity was thought to be separated from feldspar ore, and a pre-concentrate was obtained. All Fe-containing coloring impurities could not be removed due to different mineralogical origins of them in the ore. Optimum operating variables were determined as follows: 56% feed solid rate, 17° tilting angle of pinched sluice, and splitter height lower or closer to 2/3 of the total pulp film thickness. Pulp solid rate of underflow stream almost linearly changed with respect to splitter height.
PL
Albit (NaAlSi3O8) jest ważnym surowcem przemysłowym, szczególnie w ceramice i produkcji szkła. Najważniejszymi zanieczyszczeniami żelazowymi występującymi w albicie jest łuskowata mika. Celem badan było określenie możliwości wykorzystania wzbogacalnika poziomo-prądowego do wstępnego wzbogacania albitu z wykorzystaniem analizy kształtu. Badano wpływ natężenia przepływu nadawy, zawartości fazy stałej, geometrii strugi nadawy na efekt wydzielenia miki zawierającej zanieczyszczenia minerałami żelaza. Zawartość fazy stałej w nadawie została określona jako najważniejszy czynnik wpływający na efektywność procesu. Zwiększenie kąta nachylenia komory roboczej niekorzystnie wpływało na separację, szczególnie powyżej 17°. Badano wpływ rozdział miki w przekroju poprzecznym strumienia nadawy. Ziarna miki koncentrowały się w górnych warstwach strumienia. Stwierdzono, że drobne ziarna miki oddzielają się od rudy skaleniowej i można otrzymać prekoncentrat. Z uwagi na sposób występowania zanieczyszczeń nie można wydzielić wszystkich zanieczyszczeń barwiących. Określono optymalne parametry procesu: zawartość fazy stałej w nadawie 56%, kąt nachylenia rynny podawczej 17°, a wysokość rozdzielacza strugi niższa od 2/3 całkowitej grubości warstwy materiału.
Rocznik
Strony
33--38
Opis fizyczny
Bibliogr. 11 poz., tab., wykr.
Twórcy
autor
  • Muğla Sıtkı Koçman University, Mining Engineering Department, Muğla, Turkey
autor
  • Muğla Sıtkı Koçman University, Mining Engineering Department, Muğla, Turkey
autor
  • Muğla Sıtkı Koçman University, Mining Engineering Department, Muğla, Turkey
autor
  • Muğla Sıtkı Koçman University, Mining Engineering Department, Muğla, Turkey
autor
  • Muğla Sıtkı Koçman University, Mining Engineering Department, Muğla, Turkey
autor
  • Muğla Sıtkı Koçman University, Mining Engineering Department, Muğla, Turkey
Bibliografia
  • 1. AMARANTA, M.A., BOTELHO DE SOUSA, A., MACHADO LEITE, M. Beneficiation of a feldspar ore for application in the ceramic industry. The Journal of the South African Institute of Mining and Metallurgy, July/August, 1997, p. 193-196, ISSN 22256253.
  • 2. BAYRAKTAR, İ., ERSAYIN, S., GÜLSOY, Ö.Y. Magnetic separation and flotation of albite. In: Proceedings of 7th Internationa Mineral Processing Symposium, ATAK, S., ÖNAL, G., ÇELIK M.S. (Eds). Balkema, 1998, 315-318.
  • 3. ERGUN, L., ERSAYIN, S. Studies on pinched sluice concentration. Part 1: The effects of operating variables and sluice geometry on the performance of pinched sluices. Minerals Engineering, 15, 2002, p. 423-435, ISSN 0892-6875.
  • 4. HACIFAZILOĞLU, H., KURŞUN, İ., TERZI, M. Beneficiation of low-grade feldspar ore using cyclojet flotation cell, conventional cell and magnetic separator. Physicochemical Problems of Mineral Processing, 48(2): 2012, p. 381-392, ISSN 2083-3989.
  • 5. JEYADEVAN, B., SUBASINGHE, G.K.N.S. The effect of solid parameters in a pinched sluice concentrator. International Journal of Mineral Processing, 29, 1990, 31-50, ISSN 0301-7516.
  • 6. KARAGÜZEL, C., ÇOBANOĞLU, G. Stage-wise flotation for the removal of colored minerals from feldspathic slimes using laboratory scale Jameson cell. Separation and Purification Technology, 74: 2010, p. 100-107, ISSN 1383-5866.
  • 7. KING, R.P. A quantitative model for gravity separation unit operations that rely on stratification. In: APCOM 87 Proceedings of the 20th International Symposium on Computers and Mathematics in the Mineral Industries, South African Institute of Mining and Metallurgy, 1987, s. 147–151.
  • 8. MARCHAL, K.L., 2014. Geochemistry, Mineralogy and Evolution of Mica and Feldspar from within the Mount Mica Pegmatite, Maine, USA, University of New Orleans, M.Sc. Thesis., 2014, p. 130.
  • 9. OFORI-SARPONG, G., AMANKWAH, R.K. Comminution environment and gold particle morphology: Effects on gravity concentration. Minerals Engineering, 24, 2011, p. 590-592, ISSN 0892-6875.
  • 10. PIAZZA, R., BUZZACCARO, S., SECCHI, E., PAROLA, A. On the general concept of buoyancy in sedimentation and ultracentrifugation. Physical Biology, 10, 2013, p. 1-16, ISSN 1478-3967.
  • 11. VIDYADHAR, A., RAO, K.H., FORSSBERG, K.S.E. Mixed cationic/anionic collectors in the flotation separation of albite from Greek Stefania feldspar ore. 23rd International Mineral Processing Congress, İstanbul, Turkey, 2006, s. 955-962, ISBN 975-7946-27-3(Tk).
Uwagi
Opracowanie ze środków MNiSW w ramach umowy 812/P-DUN/2016 na działalność upowszechniającą naukę (zadania 2017).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-569f18ae-dc4c-49ad-a374-d7285327b2cb
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.