This paper investigates the effect of high temperatures on the compressive strength, flexural strength, and splitting tensile strength of ultra-high-performance concrete (UHPC), and ultra-high-performance, fiber-reinforced concrete (UHPFRC). The experimental variables in this study were fiber type, fiber content, and high-temperature exposure levels. Three different types of fibers were evaluated, including steel fibers, polypropylene (PP), and polyvinyl alcohol (PVA) fibers. Six concrete mixes were prepared with and without different combinations of fibers. One mix was made with no fibers. Others were made with either steel fibers alone; a hybrid of steel fibers and PVA; and a hybrid system of steel, PP, and PVA fibers. These mixes were tested under a range of temperatures and compared for strength. The UHPC and UHPFRC were exposed to high temperatures at 100°C, 300°C, 400°C, and 500°C for 3 hours. The results showed that UHPFRC did not exhibit any significant degradation when exposed to 100°C. However, reductions of approximately 18% to 25%, 12% to 22%, and 14% to 25% in the compressive strength, splitting tensile strength, and flexural strength were observed when the UHPFRC was exposed to 400°C. UHPFRC made of steel fibers showed higher mechanical properties after exposure to 400°C compared to UHPFRC made of PP and PVA fibers. The results also demonstrate the use of PVA and/or PP fibers, along with steel fiber, to withstand the effects of highly elevated temperature and prevent spalling of UHPC after exposure to elevated temperature. The observed spalling was a direct result of the melting and evaporation of PVA and/or PP fibers when exposed to high temperature, an effect that was confirmed using scanning electron microscopy.
Słowa kluczowe
Wydawca
Czasopismo
Rocznik
Tom
Strony
140--160
Opis fizyczny
Bibliogr. 78 poz., rys., tab.
Twórcy
autor
- Department of Civil Engineering, College of Engineering, King Saud University, Riyadh 1142, Saudi Arabia
autor
- Department of Civil Engineering, College of Engineering, King Saud University, Riyadh 1142, Saudi Arabia
autor
- Department of Civil and Building Engineering, University of Sherbrooke, Sherbrooke, Canada
Bibliografia
- [1] Ding M, Yu R, Feng Y, Wang S, Zhou F, Shui Z, Gao X, He Y, Chen L. Possibility and advantages of producing an ultra-high performance concrete (UHPC) with ultra-low cement content. Constr Build. Mater. 2021; 273:122023. https://doi.org/10.1016/j.conbuildmat.2020.122023.
- [2] Yu R, Spiesz P, Brouwers HJH. Development of an ecofriendly ultra-high performance concrete (UHPC) with efficient cement and mineral admixtures uses. 2014.
- [3] Li Y, Tan KH, Yang EH. Influence of aggregate size and inclusion of polypropylene and steel fibers on the hot permeability of ultra-high performance concrete (UHPC) at elevated temperature. Constr Build Mater. 2018; 169:629–637. https://doi.org/10.1016/j.conbuildmat.2018.01.105.
- [4] Arora A, Yao Y, Mobasher B, Neithalath N. Fundamental insights into the compressive and flexural response of binder- and aggregate-optimized ultra-high performance concrete (UHPC). Cem Concr Compos. 2019; 98:1–13. https://doi.org/10.1016/j.cemconcomp.2019.01.015.
- [5] Hassan M, Wille K. Experimental impact analysis on ultra-high performance concrete (UHPC) for achieving stress equilibrium (SE) and constant strain rate (CSR) in Split Hopkinson pressure bar (SHPB) using pulse shaping technique. Constr Build Mater. 2017; 144:747–757. https://doi.org/10.1016/j.conbuildmat.2017.03.185.
- [6] Yang J, Chen B, Su J, Xu G, Zhang D, Zhou J. Effects of fibers on the mechanical properties of UHPC: a review. J Traffic Transp Eng. 2022; 9:363–387. https://doi.org/10.1016/j.jtte.2022.05.001.
- [7] Meng W, Khayat K. Effect of hybrid fibers on fresh, mechanical properties, and autogenous shrinkage of cost effective UHPC. J Mater Civ Eng. 2018; 30. https://doi.org/10.1061/(ASCE)MT.1943-5533.0002212.
- [8] Xu L, Lu Q, Chi Y, Yang Y, Yu M, Y. Yan Y. Axial compressive performance of UHPC filled steel tube stub columns containing steel-polypropylene hybrid fiber. Constr Build Mater. 2019; 204:754–767. https://doi.org/10.1016/j.conbuildmat.2019.01.202.
- [9] Su Y, Li J, Wu C, Wu P, Li Z.-X. Effects of steel fibres on dynamic strength of UHPC. Constr Build Mater. 2016; 114:708–718. https://doi.org/10.1016/j.conbuildmat.2016.04.007.
- [10] Zeng X, Deng K, Liang H, Xu R, Zhao C, Cui B. Uniaxial behavior and constitutive model of reinforcement confined coarse aggregate UHPC. Eng Struct. 2020; 207:110261. https://doi.org/10.1016/j . engstruct.2020.110261.
- [11] Zhang Y, Li X, Zhu Y, Shao X. Experimental study on flexural behavior of damaged reinforced concrete (RC) beam strengthened by toughness-improved ultra-high performance concrete (UHPC) layer. Compos Part B Eng. 2020; 186:107834. https://doi.org/10.1016/j.compositesb.2020.107834.
- [12] Ghafari E, Costa H, Júlio E. RSM-based model to predict the performance of self-compacting UHPC reinforced with hybrid steel micro-fibers. Constr Build Mater. 2014; 66:375-383. https://doi.org/10.1016/j.conbuildmat.2014.05.064.
- [13] Thomas RJ, Sorensen AD. Review of strain rate effects for UHPC in tension. Constr Build Mater. 2017; 153:846-856. https://doi.org/10.1016/j.conbuildmat.2017.07.168.
- [14] Ozawa M, Subedi Parajuli S, Uchida Y, Zhou B. Preventive effects of polypropylene and jute fibers on spalling of UHPC at high temperatures in combination with waste porous ceramic fine aggregate as an internal curing material. Constr Build Mater. 2019; 206:219-225. https://doi.org/10.1016/j.conbuildmat.2019.02.056.
- [15] Yu R, Spiesz P, Brouwers HJH. Effect of nano-silica on the hydration and microstructure development of ultra-high performance concrete (UHPC) with a low binder amount. Constr Build Mater. 2014; 65:140-150. https://doi.org/10.1016/j.conbuildmat. 2014.04.063.
- [16] Qian D, Yu R, Shui Z, Sun Y, Jiang C, Zhou F, Ding M, Tong X, He Y. A novel development of green ultra-high performance concrete (UHPC) based on appropriate application of recycled cementitious material. J Clean Prod. 2020; 261:121231. https://doi.org/10.1016/J.JCLEPRO.2020.121231.
- [17] Kheir J, Klausen A, Hammer TA, De Meyst L, Hilloulin B, Van Tittelboom K, Loukili A, De Belie N. Early age autogenous shrinkage cracking risk of an ultra-high performance concrete (UHPC) wall: modelling and experimental results. Eng Fract Mech. 2021; 257:108024. https://doi.org/10.1016/j.engfracmech.2021.108024.
- [18] Li S, Tang L, Shi W, Zhong C. Experimental investigation on hydroabrasive erosion of steel fiber UHPC and rubber UHPC. Adv Mater Sci Eng. 2020; 2020:5920824. https://doi.org/10.1155/2020/5920824.
- [19] Jia L, Fang Z, Huang Z, Pilakoutas K, Wang Q, Tan X. Flexural behavior of UHPC beams prestressed with external CFRP tendons. Appl Sci. 2021; 11:9189. https://doi.org/10.3390/app11199189.
- [20] Kalifa P, Chéné G, Gallé C. High-temperature behaviour of HPC with polypropylene fibres—from spalling to microstructure. Cem Concr Res. 2001; 31:1487-1499. https://doi.org/10.1016/S0008-8846(01)00596-8.
- [21] Noumowé A, Carré H, Daoud A, Toutanji H. High-strength self-compacting concrete exposed to fire test. J Mater Civ Eng. 2006; 18:754-758. https://doi.org/10.1061/(asce)0899-1561(2006)18:6(754).
- [22] PhanL.Spalling and mechanical properties of high strength concrete at high temperature. Proc Concr under Sev Cond Fr. 2007; 1595-1608. http://fire.nist.gov/bfrlpubs/build07/art019.html (accessed December 26, 2021).
- [23] Chan SYN, X. Luo X, Sun W. Efect of high temperature and cooling regimes on the compressive strength and pore properties of high performance concrete. Constr Build Mater. 2000; 14:261-266. https://doi.org/10.1016/S0950-0618(00)00031-3.
- [24] Aslani F, Bastami M Constitutive relationships for normal-and high-strength concrete at elevated temperatures. ACI Mater J. 2011; 108:355-364. https://doi.org/10.14359/51683106.
- [25] Lau A, Anson M. Effect of high temperatures on high performance steel fibre reinforced concrete. Cem Concr Res. 2006; 36:1698-1707. https://doi.org/10.1016/j.cemconres.2006.03.024.
- [26] Varona FB, Baeza FJ, Bru D, Ivorra S. Influence of high temperature on the mechanical properties of hybrid fibre reinforced normal and high strength concrete, Constr Build Mater. 2018; 159:73-82. https://doi.org/10.1016/J.CONBUILDMAT.2017.10.129.
- [27] Mindess S, Young JF, Darwin DC. 2nd ed.; Upper Saddle River, NJ: Prentice-Hall; 2003.
- [28] Liu CT, Huang JS. Fire performance of highly flowable reactive powder concrete. Constr Build Mater. 23 (2009) 2072-2079. https://doi.org/10.1016/ j.conbuildmat.2008.08.022.
- [29] Bazant ZP, Thonguthai W. Pore pressure and drying of concrete at high temperature. ASCE J Eng Mech Div. 1978; 104:1059-1079. https://doi.org/10.1061/jmcea3.0002404.
- [30] Zohrevand P, Mirmiran P Behavior of ultrahigh-performance concrete confined by fiber-reinforced polymers. J Mater Civ Eng. 2011; 23:1727-1734. https://doi.org/10.1061/(ASCE)MT.1943-5533.0000324.
- [31] Mróz K, Hager I. Evaluation of nature and intensity of fire concrete spalling by frequency analysis of sound records. Cem Concr. Res. 2021; 148:106539. https://doi.org/10.1016/J.CEMCONRES.2021.106539.
- [32] Abadel A, Elsanadedy H, Almusallam T, Alaskar A, Abbas H, Al-Salloum Y. Residual compressive strength of plain and fiber reinforced concrete after exposure to different heating and cooling regimes. 2021; 26:6746-6765.https://doi.org/10.1080/19648189.2021.1960898.
- [33] Zhang D, Tan KH. Effect of various polymer fibers on spalling mitigation of ultra-high performance concrete at high temperature. Cem Concr Compos. 2020; 114: 103815. https://doi.org/10.1016/j.cemconcomp.2020.103815.
- [34] Travis QB, Mobasher B. Correlation of elastic modulus and permeability in concrete subjected to elevated temperatures. J Mater Civ Eng. 2010; 22:735-740. https://doi.org/10.1061/(asce)mt.1943-5533.0000074.
- [35] Gallé C, Sercombe J. Permeability and pore structure evolution of silico-calcareous and hematite high-strength concretes submitted to high temperatures. Mater Struct Constr. 2001; 34:619-628. https://doi.org/10.1617/13695.
- [36] Wille K, Naaman AE, Parra-Montesinos GJ. Ultra-high performance concrete with compressive strength exceeding 150 MPa (22 ksi): a simpler way. ACI Mater J. 2011; 108:46–54. https://doi.org/10.14359/51664215.
- [37] Richard P, Cheyrezy M. Composition of reactive powder concretes. Cem Concr Res. 1995; 25:1501–1511. https://doi.org/10.1016/0008-8846(95)00144-2.
- [38] Klingsch EW, Frangi A, Fontana M. High- and ultrahigh-performance concrete: a systematic experimental analysis on spalling. Am Concr Institute, ACI Spec. Publ. 2011; 279:269–318.
- [39] Diederichs U, Mertzsch O. Behaviour of ultra high strength concrete at high temperatures. In: Kassel, Ed. Second International Symposium on Ultra High Performance Concrete. 2008, pp. 347–354.
- [40] Peng GF, Kang YR, Huang YZ, Liu XP, Chen Q. Experimental research on fire resistance of reactive powder concrete. Adv Mater Sci Eng. 2012. https://doi.org/10.1155/2012/860303.
- [41] Varona FB, Baeza FJ, Bru D, Ivorra S. Influence of high temperature on the mechanical properties of hybrid fibre reinforced normal and high strength concrete, Constr Build Mater. 2018; 159:73–82. https://doi.org/10.1016/j.conbuildmat.2017.10.129.
- [42] Bangi MR, Horiguchi T. Effect of fibre type and geometry on maximum pore pressures in fibre-reinforced high strength concrete at elevated temperatures. Cem Concr Res. 2012; 42:459–466. https://doi.org/10.1016/J.CEMCONRES.2011.11.014.
- [43] Novák J, Kohoutková A. Fire response of hybrid fiber reinforced concrete to high temperature. Procedia Eng. 2017; 172:784–790. https://doi.org/10.1016/J.PR0ENG.2017.02.123.
- [44] Heinz D, Ludwig H-M. Heat treatment and the risk of DEF delayed ettringite formation in UHPC. In: International Symposium on Ultra High Performance Concrete in Kassel, Germany. 2004; pp. 717–730.
- [45] Chen HJ, Yu YL, Tang CW. Mechanical properties of ultra-high performance concrete before and after exposure to high temperatures. Materials (Basel). 2020; 13:770. https://doi.org/10.3390/mal3030770.
- [46] Tayeh B, Hadzima-nyarko M, Youssef M, Riad R, Defalla R, Hafez A. Behavior of ultra-high-performance concrete with hybrid synthetic fiber waste exposed to elevated temperatures. 2023; 13:129.
- [47] ISO, Elements of building construction - Part 1: General requirements. International Organization for Standardization, Geneva, Switzerland. 1999.
- [48] ASTM international, standard test method for slump of hydraulic-cement concrete. ASTM C143-10a. 2010; 13:1–4.
- [49] ASTM C138/C138M-17a, No title standard test method for density (unit weight), yield, and air content (gravimetric) of concrete. ASTM Int. 2017. https://doi.org/10.1520/C0138_C0138M-17A.
- [50] ASTM-C39, standard test method for compressive strength of cylindrical concrete. Annu B ASTM Stand. 2021; 10:1520. https://doi.org/D.O.I:10.1520/C0039_C0039M-10.
- [51] ASTM C469-02, standard test method for static modulus of elasticity and poisson’s ratio of concrete in compression. ASTM Stand. B. 2002; 04:1–5. http://portales.puj.edu.co/wjfajardo/mecanicadesolidos/laboratorios/astm/C469.pdf.
- [52] ASTM C496-96, standard test method for splitting tensile strength of cylindrical concrete specimens. Man Hydrocarb Anal 6th Ed. 2008; i:545-545–3.
- [53] A. C78/C78M-16, standard test method for flexural strength of concrete (using simple beam with third-point loading). ASTM Int. 2016. https://doi.org/10.1520/C0078_C0078M-16.
- [54] Bisby LA, Chen JF, Li SQ, Stratford TJ, Cueva , Crossling K. Strengthening fire-damaged concrete by confinement with fibre-reinforced polymer wraps. Eng Struct. 2011; 33:3381–3391. https://doi.org/10.1016/J.ENGSTRUCT.2011.07.002.
- [55] Abadel AA, Alharbi YR. Confinement effectiveness of CFRP strengthened ultra-high performance concrete cylinders exposed to elevated temperatures. Mater Sci. 2021; 39:478–490. https://doi.org/10.2478/MSP-2021-0040.
- [56] Ju Y, Wang L, Liu H, Tian K. An experimental investigation of the thermal spalling of polypropylene-fibered reactive powder concrete exposed to elevated temperatures. Sci Bull. 2015; 60:2022–2040. https://doi.org/10.1007/S11434-015-0939-0.
- [57] Novák J, Kohoutková A. Fibre reinforced concrete exposed to elevated temperature. IOP Conference Series Materials Science and Engineering. 2017; 246:012045. https://doi.org/10.1088/1757-899X/246/1/012045.
- [58] Bangi MR, Horiguchi T. Effect of fibre type and geometry on maximum pore pressures in fibre-reinforced high strength concrete at elevated temperatures. Cem Concr Res. 2012; 42:459–466. https://doi.org/10.1016/j.cemconres.2011.11.014.
- [59] Hager I, Zdeb T, Krzemié K. The impact of the amount of polypropylene fibres on spalling behaviour and residual mechanical properties of reactive powder concretes. MATEC Web Conference. 2013; 6:2003. https://doi.org/10.1051/matecconf/20130602003.
- [60] Peng GF, Chan SYN, Anson M. Chemical kinetics of C-S-H decomposition in hardened cement paste subjected to elevated temperatures up to 800°C. 2015; 13:47–52. https://doi.org/10.1680/ADCR.2001.13.2.47.
- [61] Scheinherrová L, Vejmelková E, Keppert M, Bezdička P Doleželová M, Krejsová J, Grzeszczyk S, Matuszek-Chmurowska A, Černý R. Effect of Cu-Zn coated steel fibers on high temperature resistance of reactive powder concrete. Cem Concr Res. 2019; 117:45–57. https://doi.org/10.1016/J.CEMCONRES.2018.12.008.
- [62] Ramezani M, Dehghani A, Sherif MM. Carbon nanotube reinforced cementitious composites: a comprehensive review. Constr Build Mater. 2022; 315:125100. https://doi.org/10.1016/J.CONBUILDMAT.2021.125100.
- [63] Abadel AA, Abbas H., Alshaikh IMH, Sennah K, Tuladhar R, Altheeb A, Alamri M. Experimental study on the effects of external strengthening and elevated temperature on the shear behavior of ultra-high-performance fiber-reinforced concrete deep beams. Structures. 2023; 49:943–957. https://doi.org/10.1016/j.istruc.2023.02.004.
- [64] Ambily PS, Ravisankar K, Umarani C, Dattatreya JK. Iyer NR. Development of ultra-high-performance geopolymer concrete. Concr Res. 2014; 66:82–89. https://doi.org/10.1680/macr.13.00057.
- [65] Peng NR, Bian SH, Guo ZQ, Zhao J, Peng XL, Jiang YC. Effect of thermal shock due to rapid cooling on residual mechanical properties of fiber concrete exposed to high temperatures. Constr Build Mater. 2008; 22:948–955. https://doi.org/10.1016/j.conbuildmat.2006.12.002.
- [66] Zhang P, Zhang P, Wu J, Zhang Y, Guo J. Mechanical properties of polyvinyl alcohol fiber-reinforced cementitious composites after high-temperature exposure. Gels. 2022; 8:662. https://doi.org/10.3390/ GELS8100662.
- [67] Wu Z, Shi C, He W, Wu L. Effects of steel fiber content and shape on mechanical properties of ultra high performance concrete. Constr Build Mater. 2016; 103:8–14. https://doi.org/10.1016/ J.CONBUILDMAT.2015.11.028.
- [68] Tahwia AM, Elgendy GM, Amin M. Durability and microstructure of eco-efficient ultra-high-performance concrete. Constr Build Mater. 2021; 303:124491. https://doi.org/10.1016/j.conbuildmat.2021.124491.
- [69] Gong J, Ma Y, Fu J, Hu J, Ouyang X, Zhang Z, Wang H. Utilization of fibers in ultra-high performance concrete: a review. Compos Part B Eng. 2022; 241:109995. https://doi.org/10.1016/j.compositesb.2022.109995.
- [70] Jiao C, Ta J, Niu Y, Meng S, Chen XF, He S, Ma R. Analysis of the flexural properties of ultra-high-performance concrete consisting of hybrid straight steel fibers. Case Stud Constr Mater. 2022; 17:e01153. https://doi.org/10.1016/J.CSCM.2022.E01153.
- [71] Abid M, Hou X, Zheng W, Hussain RR. High temperature and residual properties of reactive powder concrete – a review. Constr Build Mater. 2017; 147:339–351. https://doi.org/10.1016/J.CONBUILDMAT.2017.04.083.
- [72] Yoo D-Y, Banthia N, Lee J-Y, Yoon Y-S. Effect of fiber geometric property on rate dependent flexural behavior of ultra-high-performance cementitious composite. Cem Concr Compos. 2018; 86:57–71. https://doi.org/10.1016/j.cemconcomp.2017.11.002.
- [73] Yoo DY, Shin W. Improvement of fiber corrosion resistance of ultra-high-performance concrete by means of crack width control and repair. Cem Concr Compos. 2021; 121:104073. https://doi.org/10.1016/J.CEMCONCOMP.2021.104073.
- [74] Li Y, Tan KH, Yang EH. Synergistic effects of hybrid polypropylene and steel fibers on explosive spalling prevention of ultra-high performance concrete at elevated temperature. Cem Concr Compos. 2019; 96:174–181. https://doi.org/10.1016/J. CEMCONCOMP.2018.11.009.
- [75] Ozawa M, Morimoto H. Effects of various fibres on high-temperature spalling in high-performance concrete. Constr Build Mater. 2014; 71:83–92. https://doi.org/10.1016/j.conbuildmat.2014.07.068.
- [76] Xiao L, Chen P, Huang J, Peng S, Yang Z. Compressive behavior of reinforced steel-PVA hybrid fiber concrete short columns after high temperature exposure. Constr Build Mater. 2022; 342:127935. https://doi.org/10.1016/J.CONBUILDMAT.2022.127935.
- [77] Xiao J, Falkner H. On residual strength of high-performance concrete with and without polypropylene fibres at elevated temperatures. Fire Saf J. 2006; 41:115–121. https://doi.org/10.1016/J.FIRESAF.2005.11.004.
- [78] Zhang D, Tan KH, Dasari A, Weng Y. Effect of natural fibers on thermal spalling resistance of ultra-high performance concrete. Cem Concr Compos. 2020; 109:103512. https://doi.org/10.1016/j.cemconcomp.2020.103512.
Uwagi
Opracowanie rekordu ze środków MEiN, umowa nr SONP/SP/546092/2022 w ramach programu "Społeczna odpowiedzialność nauki" - moduł: Popularyzacja nauki i promocja sportu (2022-2023).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-4aa36cca-8ffb-46b5-8a74-273032399867