Experimental structural data for liquid Bi were used for estimation of the main structure parameters as well as the thermal expansion coefficient both in super cooled and superheated temperature ranges. It was shown that the equilibrium melt had a positive thermal expansion coefficient within a temperature range upon melting and a negative one at higher temperatures. The former was related to structure changes upon melting, whereas the latter with topologic disordering upon further heating. It was found that the superheated melt had a negative thermal expansion coefficient. The results obtained from structural data were compared with the thermal expansion coefficient calculated from the data of density for liquid Bi.
Słowa kluczowe
Wydawca
Czasopismo
Rocznik
Tom
Strony
767--773
Opis fizyczny
Bibliogr. 27 poz., rys., tab.
Twórcy
autor
- Physics of Metals Department, Ivan Franko National University of Lviv, 8 Kyrylo and Mephodiy St., 79005 Lviv, Ukraine
autor
- Physics of Metals Department, Ivan Franko National University of Lviv, 8 Kyrylo and Mephodiy St., 79005 Lviv, Ukraine
autor
- Physics of Metals Department, Ivan Franko National University of Lviv, 8 Kyrylo and Mephodiy St., 79005 Lviv, Ukraine
autor
- Department of Solid State Physics, Faculty of Applied Physics and Mathematics, Gdansk University of Technology, 11/12 Narutowicza St., 80-233 Gdansk, Poland
Bibliografia
- [1] In-Kook Suh, Ohta H., Waseda Y., J. Mater. Sci., 23 (1988), 757.
- [2] Ocken H., Wagner C.N. I., Phys. Rev., 1 (1966), 122.
- [3] Bar’Yakhtar V. Mikhailova L.E., Il’Inskii A.G., Romanova A.V., Khristenko T.M., JETP, 68 (5) (1989), 811.
- [4] Hongbo L., Wang X., Cao Q., Zhang D., Zhang J., Hu T., Mao H.-K., Jiang J.-Z., PNAS, 110 (25) (2013), 10068.
- [5] Crichton W.A., Mezouar M., Grande T., Stolen S., Grzechnik A., Nature, 414 (2001), 622.
- [6] McMillan P.F., Nat. Mater., 1 (2002), 19.
- [7] Yargerand J.L., Wolf G.H., Science, 306 (2004), 206.
- [8] Wilding M.C., Wilson M., McMillan P.F., Chem. Soc. Rev., 35 (2006), 964.
- [9] McMillan P.F., Wilson M., Wilding M.C., Daisenberger D., Mezouar M., Greaves N.G., J. Phys.-Condens. Mat., 19 (2007), 415101.
- [10] Cadien A., Hu Q., Meng Y., Cheng Y., Chen M., Shu J., Mao H., Sheng H., Phys. Rev. Lett., 110 (2013), 125503.
- [11] Barrett C.S., Aust. J. Phys., 13 (1960), 209.
- [12] Greenberg Y., Yahel E., Caspi E.N., Benmore C., Beuneu B., Dariel M.P., Makov G., EPL 86 (2009), 36004.
- [13] Souto J., Alemany M., Gallego L., Gonzalez L., Gonzalez D., Phys. Rev. B, 81 (2010), 134201.
- [14] Richter H., Breitling G., Adv. Phys., 16 (1968), 293.
- [15] Orton Z.B.R., Z. Naturforsch. A, 34 (1979), 1547.
- [16] Krebs H., J. Non-Cryst. Solids, 1 (1969), 455.
- [17] Davidovic M., Stojic M., Jovic D.J., J. Phys. C-Solid State Phys., 16 (1983), 2053.
- [18] Davidovic M., Stojic M., Jovic D.J., J. Non-Cryst. Solids, 61 – 62 (1984), 517.
- [19] Bellissent-Funel M.C., Bellisent R., J. Non-Cryst. Solids, 65 (1984), 383.
- [20] Matsuno N., Kamiyama H., Ishii Y., Momiuchi M., Jpn. J. Appl. Phys., 25 (1986), 275.
- [21] Momiuchi M., J. Phys. Soc. Jpn., 55 (1986), 200.
- [22] Emuna M., Mayo M., Greenberg Y., Caspi E.N., Beuneu B., Yahel E., Makov G., J. Chem. Phys., 140 (2014), 094502.
- [23] Haoran G., Chunjing S., Rui W., Xiaogang Q.I., Ning Z., Chinese Sci. Bull., 15 (2007), 2031.
- [24] Cromer D.T., Waber J.T., Acta Crystallogr., 18 (1965), 104.
- [25] Kroghmoe J., Acta Crystallogr., 9 (1956), 951.
- [26] Plevachuk Y., Sklyarchuk V., Yakymovych A., Shtablavyi I., Methods and facilities for thermophysical and structure investigations of liquid metallic alloys, in: 6th International Conference Electromagnetic Processing of Materials, Forschungszentrum, Dresden-Rossendorf-Dresden, 2009, p. 415.
- [27] Mayo M., Yahel E., Greenberg Y., Caspi E.N., Beuneu B., Makov G., J. Appl. Crystallogr., 46 (2013), 1582.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-48b5a020-1986-43ae-9ea4-b0bda887bd40