PL EN


Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników
Tytuł artykułu

Rheological and thermal properties of mixtures of hydroxyl-terminated polybutadiene and plasticizer

Treść / Zawartość
Identyfikatory
Warianty tytułu
PL
Właściwości reologiczne i termiczne mieszanin polibutadienu z końcowymi grupami hydroksylowymi oraz plastyfikatora
Konferencja
International Science-Technology Conference Armament. The Issues of Development, Production and Maintenance of Weapon Systems (21 ; 19–22.06.2017 ; Jachranka, Poland)
Języki publikacji
EN
Abstrakty
EN
Mixtures of hydroxyl-terminated polybutadiene (HTPB) and dioctyladipate (DOA) as a plasticizer, which after crosslinking are applied as binders in heterogeneous propellants, were studied.The influence of mixture composition on rheological and thermal properties, important from technological and utility viewpoint were specified. The temperature dependence of prepared mixtures viscosity were studied. Systems were subjected to crosslinking and values of pot life (tpl) were determined. It was stated that tpl rose with increasing plasticizer content. Differential scanning calorimetry and thermogravimetry techniques were used toanalyze thermal stability of mixtures. It was concluded that applied component scould not decompose in the temperature range of 290–350 K and studied mixtures did not cause the hazard of thermal explosion.
PL
Zbadano mieszaniny polibutadienu z końcowymi grupami hydroksylowymi (HTPB) oraz adypinianu dioktylu (DOA) jako plastyfikatora, które po usieciowaniu wykorzystywane są jako lepiszcza w heterogenicznych paliwach rakietowych. Określono wpływ składu na reologiczne i termiczne właściwości mieszanin, mające istotne znaczenie z technologicznego i użytkowego punktu widzenia. Zbadano zależność lepkości przygotowanych mieszanin od temperatury. Badane układy poddano sieciowaniu i wyznaczono wartości czasu życia technologicznego (tpl).Wykazano, że tpl wydłuża się ze wzrostem zawartości plastyfikatora. Stabilność termiczną mieszanin zbadano za pomocą różnicowej kalorymetrii skaningowej i termograwimetrii. Stwierdzono, że zastosowane składniki nie ulegają rozkładowi w temperaturze od 290 do 350 K i badane mieszaniny nie powodują zagrożenia eksplozją.
Czasopismo
Rocznik
Strony
53--56
Opis fizyczny
Bibliogr. 22 poz., rys.
Twórcy
autor
  • Warsaw University of Technology, Department of High-Energetic Materials, Noakowskiego 3, 00-664, Warsaw, Poland. Institute of Industrial Organic Chemistry, Annopol 6, 03-236 Warsaw, Poland
  • Institute of Industrial Organic Chemistry, Annopol 6, 03-236 Warsaw, Poland
autor
  • Warsaw University of Technology, Department of High-Energetic Materials, Noakowskiego 3, 00-664, Warsaw, Poland. Institute of Industrial Organic Chemistry, Annopol 6, 03-236 Warsaw, Poland
autor
  • Warsaw University of Technology, Department of High-Energetic Materials, Noakowskiego 3, 00-664, Warsaw, Poland. Institute of Industrial Organic Chemistry, Annopol 6, 03-236 Warsaw, Poland
Bibliografia
  • [1] Saravanakumar D., Sengottuvelan N., Narayanan V. et al.: Journal of Applied Polymer Science 2001, 119, 2517. http://dx.doi.org/10.1002/app.32859
  • [2] Czub P., Kasza P.: Polimery 2014, 59, 466. http://dx.doi.org/10.14314/polimery.2014.466
  • [3] Kozakiewicz J., Rokicki G., Przybylski J. et al.: Polimery 2011, 56, 564.
  • [4] Chai T., Liu Y.C., Ma H. et al.: “Rheokinetic analysis on the curing process of HTPB-DOA-MDI binder system”, IOP Conference Series: Materials Science and Engineering, IOP Publishing, Hangzhau, China, 20–23 May 2016, p. 1.
  • [5] Chaturvedi S., Dave P.N.: Arabian Journal of Chemistry 2015. http://dx.doi.org/10.1016/j.arabjc.2014.12.033
  • [6] Cao Z., Zhou Q., Jie S. et al.: Industrial & Engineering Chemistry Research 2016, 55, 1582. http://dx.doi.org/10.1021/acs.iecr.5b04921
  • [7] Yang L., Xie K., Pei J. et al.: Journal of Applied Polymer Science 2016, 133, 43 512. https://dx.doi.org/10.1002/app.43512
  • [8] Tanver A., Rehman F., Wazir A. et al.: RSC Advances 2016, 6, 11 032. http://dx.doi.org/10.1039/C5RA23250C
  • [9] Kumari D., Balakshe R., Banerjee S. et al.: Review Journal of Chemistry 2012, 2, 240. http://dx.doi.org/10.1134/S207997801203003X
  • [10] Florczak B., Bednarczyk E., Maranda A.: Chemik 2015, 69, 136.
  • [11] Florczak B., Bogusz R., Skupiński W. et al.: Central European Journal of Energetic Materials 2015, 12, 841.
  • [12] Singh M., Kanungo B.K., Bansal T.K.: Journal of Applied Polymer Science 2002, 85, 842. http://dx.doi.org/10.1002/app.10719
  • [13] Saeb M.R., Rastin H., Nonahal M. et al.: Journal of Applied Polymer Science 2017, 134, 45 221. http://dx.doi.org/10.1002/app.45221
  • [14] Sekkar V., Alex A.S., Kumar V. et al.: Journal of Macromolecular Science, Part A 2017, 54, 171. http://dx.doi.org/10.1080/10601325.2017.1265403
  • [15] Bandgar B.M., Sharma K.C., Mukundan T. et al.: Journal of Applied Polymer Science 2003, 89, 1331. http://dx.doi.org/10.1002/app.12254
  • [16] Sekkar V., Raunija T.S.K.: Propellants, Explosives, Pyrotechnics 2015, 40, 267. http://dx.doi.org/10.1002/prep.201400054
  • [17] Xu Z.-X., Wang Q., Fu X.-Q.: Journal of Hazardous Materials 2015, 300, 702. http://dx.doi.org/10.1016/j.jhazmat.2015.07.069
  • [18] Gańczyk K., Zygmunt A., Gołofit T.: Journal of Thermal Analysis and Calorimetry 2016, 125, 967. http://dx.doi.org/10.1007/s10973-016-5476-9
  • [19] Gołofit T., Zyśk K.: Journal of Thermal Analysis and Calorimetry 2015, 119, 1931. http://dx.doi.org/10.1007/s10973-015-4418-2
  • [20] Gołofit T., Książczak A.: Problemy Mechatroniki: Uzbrojenie, Lotnictwo, Inżynieria Bezpieczeństwa 2011, 2, 31.
  • [21] Semenov N.N.: “Chemical Kinetics and Chain Reactions”, Oxford University Press, London 1935, p. 489.
  • [22] Cepeda E., Hermosa M., Llorens F. et al.: International Journal of Food Science and Technology 2002, 37, 271. http://doi.org/10.1046/j.1365-2621.2002.00566.x
Uwagi
PL
Opracowanie rekordu w ramach umowy 509/P-DUN/2018 ze środków MNiSW przeznaczonych na działalność upowszechniającą naukę (2018).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-2d84b57b-c79c-47de-9c82-4ac16ae82a7d
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.