Stability of a Lamellar Structure - Effect of the True Interlamellar Spacing on the Durability of a Pearlite Colony

Treść / Zawartość
Identyfikatory
Warianty tytułu
PL
Stabilność struktury płytkowej - Wpływ rzeczywistej odległości międzypłytkowej na trwałość kolonii perlitu
Języki publikacji
EN
Abstrakty
EN
A lamellar microstructure is, beside a granular and dispersive one, the most frequently observed microstructure in the case of metal alloys. The most well-known lamellar microstructure is pearlite, a product of a eutectoidal transformation in the Fe-Fe3C system. The lamellar morphology of pearlite - cementite and ferrite lamellae placed interchangeably within one structural unit described as a colony - is dominant. The durability of the lamellar morphology is much diversified: in the microstructure of spheroidizingly annealed samples, one can observe areas in which the cementite is thoroughly spheroidized, next to very well-preserved cementite lamellae or even whole colonies of lamellar pearlite. The mentioned situation is observed even after long annealing times. The causes of such behaviour can vary. The subject of the previous work of the authors was the effect of the orientation between the ferrite and the cementite on the stability of the lamellar morphology. This work constitutes a continuation of the mentioned paper and it concerns the effect of the true interlamellar spacing on the stability of the lamellar morphology of cementite.
PL
Mikrostruktura płytkowa to obok ziarnistej i dyspersyjnej jedna z najczęściej spotykanych w przypadku stopów metali. Najbardziej znaną mikrostrukturą płytkową jest perlit, produkt przemiany eutektoidalnej w układzie Fe-Fe3C. Morfologia płytkowa perlitu –płytki ferrytu i cementytu ułożone na przemian w obrębie jednej jednostki strukturalnej określanej mianem kolonii - jest dominująca. Trwałość morfologii płytkowej jest bardzo zróżnicowana - w mikrostrukturze próbek wyżarzanych sferoidyzująco obserwuje się obszary, w których cementyt jest zupełnie zesferoidyzowany obok bardzo dobrze zachowanych płytek cementytu lub wręcz całych kolonii perlitu płytkowego. Opisana sytuacja ma miejsce nawet po długich czasach wyżarzania. Przyczyny takiego zachowania mogą być różne. Przedmiotem wcześniejszej pracy autorów był wpływ orientacji pomiędzy ferrytem a cementytem na stabilność morfologii płytkowej. Niniejszy artykuł stanowi kontynuację pracy wspomnianej wcześniej i dotyczy wpływu rzeczywistej odległości międzypłytkowej na stabilność morfologii płytkowej cementytu.
Twórcy
autor
  • AGH University of Science and Technology, Department of Physical and Powder Metallurgy, Faculty of Metals Engineering and Industrial Computer Science, Al. Mickiewicza 30, 30-059 Kraków, Poland
autor
  • AGH University of Science and Technology, Department of Physical and Powder Metallurgy, Faculty of Metals Engineering and Industrial Computer Science, Al. Mickiewicza 30, 30-059 Kraków, Poland
  • AGH University of Science and Technology, Department of Physical and Powder Metallurgy, Faculty of Metals Engineering and Industrial Computer Science, Al. Mickiewicza 30, 30-059 Kraków, Poland
Bibliografia
  • [1] M. Hillert, The formation of pearlite, in: V. F. Zakay, H. I. Aaronson (Eds.), Decomposition of austenite by diffusional processes, New York, NY Interscience 1962.
  • [2] S. A. Hackney, G. J. Shiflet, Acta Metall. 35, 1019-1028 (1987).
  • [3] S. N. Doi, H. J. Kestenbach, Metallography 23, 135-146 (1989).
  • [4] T. Kozieł, P. Matusiewicz, M. Kopyściański, A. Zielińska-Lipiec, Metallurgy and Foundry Engineering 39, 7-14 (2013).
  • [5] B. Pawłowski, P. Bała, J. Krawczyk, Metallurgy and Foundry Engineering 35, 121-128 (2009).
  • [6] J. W. Martin, R. D. Doherty, Stability of Microstructure in Metallic Systems, Cambridge University Press 1976.
  • [7] M. McLean, Metal Science 3, 113-122 (1978).
  • [8] F. A. Nichols, W. W. Mullins, Transactions of Metallurgical Society of AIME 233, 1840-1848 (1965).
  • [9] Y. L. Tian, R.W. Kraft, Metallurgical Transaction A 18A, 1403-1414 (1987).
  • [10] A. A. Baranow, Izwiestia Akademii Nauk SSSR. Metałły 3 104-107 (1969).
  • [11] D. Goodchild, Scandinavian Journal of Metallurgical 1, 235 - 240 (1972).
  • [12] W. W. Mullins, Journal of Applied Physics 28, 333-339 (1957).
  • [13] G. H. Nijhof, Härterei Techn. Mitt. 35, 59-68 (1980).
  • [14] G. H. Nijhof, Härterei Techn. Mitt. 36, 242-247 (1981).
  • [15] Y. L. Tian, R. W. Kraft, Metallurgical Transaction A 18A, 1359-1369 (1987)
  • [16] T. Skowronek, A. Czarski, K. Satora, Materiały XXX Szkoły Inżynierii Materiałowej, Kraków Ustroń-Jaszowiec 205-209 (2002).
  • [17] R. T. DeHoff, F. N. Rhines, Quantitative Microscopy, New York, McGraw-Hill 1968.
  • [18] E. E. Underwood, Quantitative Stereology, Addison-Weseley 1970.
  • [19] A. Czarski, J. Ryś, Acta Stereologica 6, 567-572 (1987).
  • [20] A. Czarski, P. Matusiewicz, Metallurgy and Foundry Engineering 41, (2015) (will be published).
  • [21] A. Czarski, E. Głowacz, Archives of Metallurgy and Materials 55, 101-105 (2010).
  • [22] J. Ryś, A. Czarski, Proc. of IV Symposium on Metallography, Vysoke Tatry, Czechoslovakia 1, 25-30 (1986).
  • [23] A. Czarski, P. Matusiewicz, Metallurgy and Foundry Engineering 38, 133-137 (2012).
  • [24] A. Czarski, J. Ryś, Pr. Kom. Metal.-Odlew., Pol. Akad. Nauk- Oddz. Krakow, Metalurgia 35, 35-42 (1988).
  • [25] P. Matusiewicz, A. Czarski, H. Adrian, Metallurgy and Foundry Engineering 33, 33-40 (2007).
  • [26] A. Czarski, T. Skowronek, W. Osuch, Metallurgy and Foundry Engineering, 33, 41-49 (2007).
  • [27] T. Skowronek, W. Ratuszek, K. Chruściel, A. Czarski, K. Satora, K. Wiencek, Archives of Metallurgy and Materials 49, 961-971 (2004)
Uwagi
PL
Opracowanie ze środków MNiSW w ramach umowy 812/P-DUN/2016 na działalność upowszechniającą naukę.
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-2cb60acd-21ee-4c21-b259-3cc856c1a148
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.