Changes of crystallite sizes in the oxide layer forming during long-term operation of 10CrMo9-10 steel

Autorzy
Treść / Zawartość
Identyfikatory
Warianty tytułu
Języki publikacji
EN
Abstrakty
EN
The paper contains results of the studies on X-ray diffraction analysis XRD (studying the phase composition, crystallite sizes) of oxide layers on 10CrMo9-10 steel, operated for a long time at an elevated temperature (T = 525°C, t = 200,000 h). The oxide layer was studied on a surface and a cross-section at the outer on the inlet both on the fire and counter-fire side of the tube wall surface. X-ray studies were carried out on the outer surface of a tube, and then the layer surface was polished down and the diffraction measurements were performed again to determine crystallite size in oxide layers. Based on the width and the position of the main coat and substrate reflections, the size of the crystallites was determined using the Scherrer formula.
Rocznik
Tom
Strony
289--296
Opis fizyczny
Bibliogr. 15 poz., rys., wykr., zdj.
Twórcy
autor
  • Institute of Materials Engineering, Faculty of Production Engineering and Materials Technology, Czestochowa University of Technology, ul. Armii Krajowej 19, 42-200 Częstochowa
Bibliografia
  • ANTONOV M., VEINTHAL R., HUTTUNEN-SAARIVIRTA E., HUSSAINOVA I., VALLIKIVI A., LELEIS M., PRISS J. 2013. Effect of oxidation on erosive wear behaviour of boiler steels. Tribology International, 68: 35–44.
  • BISCHOFF J., MOTTA A.T., EICHFELD C., COMSTOCK R.J., CAO G., ALLEN T.R. 2013. Corrosion of ferritic-martensitic steels in steam and supercritical water. Journal of Nuclear Materials, 441: 604–611.
  • FRANGINI S., MASCI A., MCPHAIL S.J., SOCCIO T., ZAZA F. 2014. Degradation behavior of a commercial 13Cr ferritic stainless steel (SS405) exposed to an ambient air atmosphere for IT-SOFC interconnect applications. Materials Chemistry and Physics, 144: 491–497.
  • GAWRON P., DANISZ S. 2012. Dostosowanie zakresu badań diagnostycznych wybranych elementów kotłów pracujących w warunkach współspalania biomasy. Energetyka, 702(12): 843–853.
  • GWOŹDZIK M. 2013. Utlenianie stali 10CrMo9-10 podczas eksploatacji w wysokiej temperaturze. Inżynieria Powierzchni, 1: 36–39.
  • GWOŹDZIK M. 2014. Mechanizm degradacji warstw tlenkowych na stalach długotrwale eksploatowanych w energetyce. Monografia, 291, Wydawnictwo Politechniki Częstochowskiej.
  • GWOŹDZIK M. 2016. Analysis of Crystallite Size Changes in an Oxide Layer Formed on Steel Used in the Power Industry. Acta Physica Polonica A, 130(4): 935–938.
  • KLEPACKI F., WYWROT D. 2010. Trwałość wężownic przegrzewaczy wtórnych w warunkach niskoemisyjnego spalania. Energetyka, 678(12): 816–820.
  • KLEPACKI F. 2006. Korozja wysokotemperaturowa wężownic przegrzewaczy kotłów. Energetyka, 621(3): 197–200.
  • KULESZA S., BRAMOWICZ M. 2014. A comparative study of correlation methods for determination of fractal parameters in surface characterization. Applied Surface Science, 293: 196–201.
  • LABISZ K. 2014. Microstructure and mechanical properties of high power diode laser (HPDL) treated cast aluminium alloys. Mat.-wiss. U. Werkstofftech, 45(4): 314–324.
  • LABISZ K. 2015. Influence of Laser Feeding on Structure and Properties of Cast Aluminium Alloy Surface. In: Mechanical and Materials Engineering of Modern Structure and Component Design. Eds. A. Öchsner, H. Altenbach. Advanced Structured Materials, 70. Springer, Cham, p. 317–343.
  • PRISS J., ROJACZ H., KLEVTSOV I., DEDOV A., WINKELMANN H., BADISCH E. 2014. High temperature corrosion of boiler steels in hydrochloric atmosphere under oil shale ashes. Corrosion Science, 82: 36–44.
  • SZAFARSKA M., IWASZKO J. 2012. Laser remelting treatment of plasma-sprayed Cr2O3 oxide coatings. Archives of Metallurgy and Materials, 57(1): 215–221.
  • ŢǍLU Ş., BRAMOWICZ M., KULESZA S., SHAFIEKHANI A., GHADERI A., MASHAYEKHI F., SOLAYMANI S. 2015. Microstructure and Tribological Properties of FeNPs@a-C:H Films by Micromorphology Analysis and Fractal Geometry. Industrial & Engineering Chemistry Research, 33 (54): 8212–8218.
Uwagi
Opracowanie w ramach umowy 509/P-DUN/2018 ze środków MNiSW przeznaczonych na działalność upowszechniającą naukę (2018).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-2852c2eb-9037-4d95-b1fb-f2cae4c79eb5
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.