In this investigation the surface of an aluminized sample of plain carbon steel was melted and alloyed using a tingsten inert gas (TIG) welding process to produce iron-aluminide intermetallic phases on the surface. The produced coating was then characterized by SEM and EDS and its high-temperature properties in O2 + 1%SO2 gas were examined. The results showed that the Fe3 Al coating produced could protect the substrate as it was subjected to the corroding gases at 700°C due to the formation of an alumina layer between the substrate and an outer layer of Fe2 O3 . At 900°C, the coating could only protect the substrate for 64 h. The lack of further protection at this temperature is attributed to the decrease in the protective properties of alumina with an increase in its temperature and the lack of presence of enough Al atoms in the coating for the repair of the defects formed in the alumina layer.
Słowa kluczowe
Wydawca
Czasopismo
Rocznik
Tom
Strony
529--538
Opis fizyczny
Bibliogr. 31 poz., fot., rys., tab.
Twórcy
autor
- Hahid Bahonar University of Kerman, Faculty of Engineering, Department of Metallurgy and Materials Science, Kerman, Iran
autor
- Hahid Bahonar University of Kerman, Faculty of Engineering, Department of Metallurgy and Materials Science, Kerman, Iran
autor
- Tarbiat Modares University, Faculty of Engineering, Materials Science and Engineering Department, Jalal Ale Ahmad Highway, 14115-111 Tehran, Iran
Bibliografia
- [1] P. Fan, E. Riddle, Z. Z. Fang, H. Y. Sohn, Surf. Coat. Technol. 202, 6090-6094 (2008).
- [2] M. Emami, H. R. Shahverdi, S. Hayashi, M. J. Torkamany, Metall. Mater. Trans. A 44, 3176-3184 (2013).
- [3] W. J. Cheng, C. J. Wang, Mater. Charact. 69, 63-70 (2012).
- [4] S. F. Corbin, E. Toyserkani, A. Khajepour, Mater. Sci. Eng. A 354, 48-57 (2003).
- [5] Y. Zhang, B. A. Pint, G. W. Garner, K. M. Cooley, J. A. Haynes, Surface and Coatings Technology, 188-189, 35-40 (2004).
- [6] Y. Zhang, B. A. Pint, K. M. Cooley, J. A. Haynes, Surf. Coat. Technol. 200, 1231-1235 (2005).
- [7] M. Emami, S. M. M. Hadavi, S. Hayashi, H. R. Shahverdi, Oxid. Met. 80, 437-451(2013).
- [8] N. I. Jamnapara, S. Frangini, J. Alphonsa, N. L. Chauhan, S. Mukherjee, Surf. Coat. Technol. 266, 146-150 (2015).
- [9] C. Christoglou, N. Voudouris, G. N. Angelopoulos, Surf. Coat. Technol. 155, 51-58 (2002).
- [10] Y. Q. Wang, Y. Zhang, D. A. Wilson, Surf. Coat. Technol. 204, 2737-2744 (2010).
- [11] M. H. Sohi, M. Ebrahimi, H. M. Ghasemi, A. Shahripour, Appl. Surf. Sci. 258, 7348-7353 (2012).
- [12] S. Buytoz, M. Ulutan, Surf. Coat. Technol. 200, 3698-3704 (2006).
- [13] P. Omranian Mohammadi, R. Raiszadeh, H. Shahverdi, Int. J. Adv. Manuf. Technol. 96, 1655-1663 (2018).
- [14] A. Amirsadeghi, M. H. Sohi, J. Mater. Process. Technol. 201, 673-677 (2008).
- [15] A. Amirsadeghi, M. H. Sohi, S. F. Bozorg, J. Iron. Steel Res. Int. 15, 86-94 (2008).
- [16] M. Eroğlu, N. Özdemir, Surf. Coat. Technol. 154, 209-217 (2002).
- [17] O. N. Çelik, M. Ulutan, H. Gaşan, Ü. Er, S. Buytoz, Surf. Coat. Technol. 206, 1423-1429 (2011).
- [18] A. S. Khanna, Introduction to high temperature oxidation and corrosion, 2002 ASM International.
- [19] P. Kofstad, R. Bredesen, Solid State Ionics. 52, 69-75 (1992).
- [20] W. H. Lee, R. Y. Lin, Mater. Chem. Phys. 58, 231-242 (1999).
- [21] V. S. Rao, R. G. Baligidad, V. S. Raja, Intermetallics. 10, 73-84 (2002).
- [22] W. F. Gale, T. C. Totemeier, Smithells metals reference book, 2003 Elsevier.
- [23] V. S. Rao, V. Raja, Intermetallics. 11, 119-128 (2003).
- [24] H. Bartar Esfahani, R. Raiszadeh, H. Doostmohammadi, Metall. Mater. Trans. A 47, 1331-1338 (2016).
- [25] F. Najafzadeh-Bakhtiarani, R. Raiszadeh. J. Mater. Sci. 46, 1305-1315 (2010).
- [26] R. Raiszadeh, W. D. Griffiths, Metall. Mater. Trans. B 42, 133-143 (2011).
- [27] O. Milton, Engineering Materials Science, 1995 San Diego: Academic Press.
- [28] N. B. Pilling, R. E. Bedsworth, J. Inst. Met. 29, 529-591(1923).
- [29] R. Y. Chen, W. Y. D. Yeun, Oxid. Met. 59, 433-468 (2003).
- [30] L. Yajiang, W. Juan, Y. Yansheng, M. Haijun, Bull. Mater. Sci. 28, 69-74 (2005).
- [31] W. C. Sleppy, J. Electrochem. Soc. 108, 1097-1102 (1961).
Uwagi
PL
Opracowanie rekordu ze środków MNiSW, umowa Nr 461252 w ramach programu "Społeczna odpowiedzialność nauki" - moduł: Popularyzacja nauki i promocja sportu (2020).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-1e7045ea-847d-48a0-9cf4-59697541a38f