For the reliable applications of silver nanowires, AgNW, which is used as a conductive transparent film in electronic devices, the isothermal degradation behaviors of AgNW films with and without overcoating were investigated. Accelerated isothermal degradation was performed as a function of temperature, time, and atmosphere. Electrical resistance and optical transmittance were measured and correlated with the microstructural damages, such as formation of oxide particles and fragmentations of AgNW, which were quantitatively determined from the scanning electron micrographs. The overcoating retarded the formation of oxide particles and subsequent fragmentations as well as resulting degradation in electrical resistance without affecting the optical transmittance.
Twórcy
autor
  • Seoul National University of Science and Technology, Program of Materials Science & Engineering, Convergence Institute of Biomedical Engineering and Biomaterials, Seoul, 01811, Korea
  • Seoul National University of Science and Technology, Department of Materials Science & Engineering, Seoul, 01811, Korea
autor
  • Seoul National University of Science and Technology, Department of Materials Science & Engineering, Seoul, 01811, Korea
autor
  • Seoul National University of Science and Technology, Department of Materials Science & Engineering, Seoul, 01811, Korea
autor
  • Korea Institute of Materials Science, Material Testing & Reliability Division, Changwon, 51508, Korea
  • Seoul National University of Science and Technology, Department of Materials Science & Engineering, Seoul, 01811, Korea
Bibliografia
  • [1] C. H. Liu, X. Yu, Nanoscale Res. Lett. 6 (1), 75-82 (2011).
  • [2] M. Bobinger, D. Angeli, S. Colasanti, P. L. Torraca, L. Larcher, P. Lugli, Physica. Status. Solidi. A 214 (1), 1600466 (2017).
  • [3] J. Jiu, J. Wang, T. Sugahara, S. Nagao, M. Nogi, H. Koga, K. Suganuma, M. Hara, E. Nakazawa, H. Uchida, RSC Adv. 5, 27657-27664, (2015).
  • [4] P. Blake, P. D. Brimicombe, R. R. Nair, T. J. Booth, D. Jiang, F. Schedin, L. A. Ponomarenko, S. V. Morozov, H. F. Gleeson, E. W. Hill, A. K. Geim, K. S. Novoselov, Nano Letters 8 (6), 1704-1708, (2008).
  • [5] H. H. Khaligh, I. A. Goldthorpe, Nanoscale 8 (1), 235, (2013).
  • [6] D. C. Choo, T. W. Kim, Scientific Reports 7 (1), 1696, (2017).
  • [7] G. Deignan, Corrosion study of silver nanowires, Master thesis, University of Waterloo, Canada 2017.
  • [8] H. Y. Kim, Mechanical and thermal degradation of AgNW film, Master thesis, Seoul National University of Science and Technology, Korea 2018.
  • [9] A. E. Abbass, A. J. V. Vuuren, H. C. Swart, R. E. Kroon, Journal of Non-Crystalline Solids 475, 71-75, (2017).
Uwagi
EN
1. This work was financially supported by KIMS (Korea Institute of Materials Science, South Korea, Project No.: PNK 5780)
PL
2. Opracowanie rekordu w ramach umowy 509/P-DUN/2018 ze środków MNiSW przeznaczonych na działalność upowszechniającą naukę (2019).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-014a3cd8-d661-42ad-883d-889eb74cc10c
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.