EN
The aim of this study was to analyze the impact of the type and thickness of selected polyurethane foams on the comfort of furniture use. The utilitarian objective included development of dependence catalogue of the comfort of polyurethane foams on their type and thickness. The comfort of polyurethane foams was determined using a sensory mat. Obtained results from determinations were elaborated and presented in tables and graphs. The conclusions stated that the best material (the most comfortable in use) for a woman is VP 3545 foam with a thickness of 40 mm and for man VP 2840 foam with a thickness of 90 mm and the dependence catalogue of polyurethane foams on their type and thickness were prepared.
EN
A computational model based on the equation of damped longitudinal wave for the Kelvin-Voigt model (e.g. [8]) is presented in the paper. A results of ultrasonic tests of wooden samples are also presented. The presented mathematical model and the test results allowed estimating values of the modulus of elasticity and the viscosity coefficient of wood for the Kelvin-Voigt model. The results are compared with the values of the parameters determined in work [7].
PL
Określono wpływ impregnacji drewna na jego wybrane właściwości mechaniczne. Przeprowadzono nieniszczące badania i analizę drgań swobodnych belek z drewna niezaimpregnowanego i zaimpregnowanego. Właściwości mechaniczne opisano z wykorzystaniem modelu Kelvina-Voigta. Przedstawiono opis drgań swobodnych w przypadku tego modelu oraz wyniki badań.
EN
A effect of wood preservation on the selected mechanical properties was determined. A non-destructive testing consisting in the analysis of the free vibration of beams of nonimpregnated and impregnated wood were carried out. Mechanical properties were described using Kelvin-Voigt model. A description of the free vibration in this model and the results of the tests were presented.
4
Content available remote Szacowanie funkcji relaksacji warstw drewna – analiza wrażliwości modelu
EN
In the paper a analysis enabling the evaluation the stability and the usefulness of the model described in [1] was presented. The analysis was carried out for plywood and solid wood
5
Content available remote Wpływ wilgotności na sztywnościowe tłumienie drgań konstrukcji drewnianych
EN
The paper presents the results of dynamic tests of wooden cantilever beam at different humidities. It shows the influence of moisture content on stiffness damping. The model of stiffnes-mass damping is used in the considerations.
EN
In order to investigate the phase constitution of the nanocrystalline Nd9.5Fe63.65B21.85Nb5 alloy ribbons in the as-cast state and after short-time annealing Mossbauer study has been carried out. In as-cast state, ribbon samples were not fully amorphous but revealed soft magnetic properties. X-ray diffraction analysis showed the presence of hard magnetic Nd2Fe14B, metastable Nd2Fe23B3 and paramagnetic Nd1+epsilonFe4B4 phases in annealed samples. Mossbauer spectroscopy was used to determine the fractions of constituent phases formed during annealing of ribbons. Magnetic measurements were made with a vibrating sample magnetometer (VSM) and have shown that with increasing annealing temperature the remanence polarization Jr and maximum energy product (BH)max values were increasing.
PL
W artykule przedstawiono technologię i wyniki eksperymentalne światłowodowego czujnika temperatury progowej zbudowanego na bazie wypełnionego substancją organiczną włókna mikrostrukturalnego. Do konstrukcji czujnika wybrano najprostszą konfigurację natężeniowego czujnika światłowodowego. Czujnik składa się ze źródła światła, patchcordu światłowodowego z wypełnionym włóknem mikrostrukturalnym oraz fotodetektora. Patchcord światłowodowy będący optodątego czujnika to częściowo wypełniony odcinek włókna mikrostrukturalnego wspawany pomiędzy dwa odcinki standardowego włókna światłowodowego. Mieszanina wypełniająca został przygotowana tak, aby zmiany temperatury w czasie ogrzewania lub chłodzenia wypełnionej części włókna zmieniały jej współczynnika załamania dając w efekcie zerowe natężenie wiązki świetlnej poniżej temperatury progowej oraz dużą wartość tego natężenia powyżej tej temperatury. Efekt skokowej zmiany współczynnika załamania wypełniającej substancji organicznej osiągany jest w trakcie jej zmiany stanu skupienia ze stałej na ciekłą. Dzięki temu możliwe jest rozróżnienie stanu włączenia dla niskiego współczynnika załamania cieczy oraz stanu wyłączenia dla wysokiego współczynnika załamania substancji w stanie stałym.
EN
Variable optical attenuators (VOAs) play an important role in optical communications as equalizers for dynamic channel power and wavelength division multiplexing in a transmission system. Controlling and monitoring of optical power are also necessary in sensing applications, and especially, in optical systems which require high power laser operation or critical temperature threshold monitoring. Various types of VOA have been developed based on different mechanisms, such as bending loss control, light leaking from the fibre cladding, temperature tuning of the polymer incorporated into the tapered microstructured fibre or electrical tuning of the liquid crystal layers.In this paper we would like to discuss the highly dynamic VOA based on a tuneable microstructured fibre filled with different chemical mixtures used as an on/off temperature switch. Furthermore, the technology of low loss coupling and splicing of the applied MSF with a standard single mode fibre has been developed. Therefore, in the proposed application an optical signal can be transmitted to and from the switch by a standard telecom fibre which considerably reduces transmission losses and allows for the use of standard off-the-shelf components reducing costs of the overall system.
PL
Właściwości włókien mikrostrukutralnych takie jak: jednomodowe prowadzenie światła w szerokim zakresie spektralnym (od ultrafioletu do podczerwieni), bardzo wysoka dwójłomność, bardzo duże lub bardzo małe pole modu są przedmiotem badań wielu zespołów naukowych na świecie. Właściwości te wynikają przede wszystkim z rozmiaru, kształtu oraz lokalizacji otworów powietrznych w strukturze włókna mikrostrukturalnego. Zmiana tych parametrów pozwala na zastosowania takich włókien do różnych aplikacji. Sprawia to rosnące zainteresowanie włóknami mikrostrukturalnymi które widoczne jest w powstających czujnikach opartych na ich bazie - m. in. Czujniki interferometryczne do detekcji rozmaitych parametrów fizycznych. Jednym z takich czujników jest światłowodowy interferometr Macha-Zehndera wykorzystujący jako gałąź czujnikową włókno mikrostrukturalne. Interferometr ten jest jednym z układów który nie został opisany w fachowej literaturze. Czujnik zbudowany w oparciu o taki interferometr może być użyty do pomiarów wibracji, dynamicznego lub statycznego nacisku, rozciągania lub skręcania. W pracy tej przedstawione zostało porównanie czułości temperaturowej oraz mechanicznej włókien mikrostrukturalnych ze standardowymi włóknami jednomodowymi. Do tego celu wykorzystaliśmy interferometr Macha- Zehndera z wymiennym ramieniem czujnikowym. Zastosowanie takiego rozwiązania pozwoliło na zbadanie wielu światłowodów w jednym układzie pomiarowym. Czułość temperaturowa jest najistotniejszym czynnikiem przy projektowaniu czujników. Włókna mikrostrukturalne zbudowane są z czystego szkła krzemiankowego z heksagonalną macierzą otworów powietrznych co powoduje brak naprężeń termicznych pomiędzy płaszczem a rdzeniem jak w przypadku włókien z domieszkowanym rdzeniem.
EN
Microstructured fibres (MSFs) reveal unique properties including endlessly single-mode operation from ultraviolet to infrared wavelengths, very high birefringence or nonlinearity, very large or very small effective mode field area, and many others. The size, shape and the location of the air holes allow for tailoring MSF parameters in a very wide range, way beyond the classical fibres, what opens up the possibilities for various applications. Due to their advantages MSFs obtain growing attention for their perspectives in sensing applications. Different MSF sensors have already been investigated, including interferometrie transducers for diverse physical parameters. Until now, there have not been any publications reporting on the sensing applications of MSF Mach-Zehnder interferometers, targeting the mechanical measurements of vibrations, dynamic or static pressure, strain, bending and lateral force. Moreover, a critical feature opening the prospective of optical fibre transducer to successfully accomplish a particular sensing task remains its cross-sensitivity to temperature. Studied MSF is made of pure silica glass in the entire cross-section with a hexagonal structure of the holes. Consequently, there is no thermal stress induced by the difference in thermal expansion coefficients between the doped core region and the pure silica glass cladding, in contrast to standard fibres.
EN
A microorganisms change considerably the rheological properties of wood. The main objective of the paper is to analyze the usefulness of model to estimate the effects of such damage on the process of creep of wood.
10
Content available remote Proces pełzania drewna zaatakowanego przez mikroorganizmy
EN
The results of creep test for wood attacked by fungus are presented in the paper. They show that destruction caused by microorganisms intensifies rheological processes. Also values of the creep parameters for wood damaged by fungus are estimated.
EN
In the paper equation of strain in process of wood creep is derived. The wood is treated as polymer because is composed of cellulose in the main.
EN
In the paper results of test of wood creep was presented. Creep function of wood at pure bending was also determined.
13
Content available remote The evolution of microstructure in annealed LaFeSi-type alloys
EN
The evolution of microstructure and the phase constitution of the LaFe11.0Co0.8(Si0.4Al0.6)1.2 alloy in as-cast state and after subsequent annealing at 1323 K for 10, 20, 49 days was studied. In the LaFe11.0Co0.8(Si0.4 Al0.6)1.2 alloy after arc-melting, the dominant dendritic ?-Fe phase crystallizes, which is confirmed by X-ray diffraction. Annealing of the samples resulted in evolution of microstructure and the phase constitution. Prolonged annealing of the samples causes almost full homogenization of the alloy with the single-phase structure identified as La(Fe0.85Co0.06Si0.04Al0.05)13 phase of the NaZn13-type structure.
PL
W pracy określono gęstość energii ścian domenowych w kilku grupach jednoosiowych ferromagnetyków: UFe10-xNixSi2 (x=0, 2, 4); UFe12-xAlxSi2 (x=1, 6); R2Fe14B (R=Pr, Nd, Gd, Dy); RMn2Ge2 (R=La, Ce, Pr, Nd) oraz Sm2Fe17N3, stosując stereologiczną metodę Bodenbergera-Huberta. Magnetyczną strukturę domenową obserwowano wykorzystując metodę figur proszkowych (ferrofluid). Ujawniona struktura domenowa jest typowa dla magnesów o jednym kierunku łatwego namagnesowania i dużej wartości anizotropii magnetokrystalicznej. Wyznaczone wartości gestości energii ścian domenowych porównano z wynikami literaturowymi otrzymanymi innymi metodami i stwierdzono dobrą zgodność.
EN
In the paper domain wall energy density for some groups of uniaxial magnetic materials: UFe10-xNixSi2 (x=0, 2, 4), UFe12-xAlxSi2 (x=1, 6), R2Fe14B (R=Pr, Nd, Gd, Dy), RMn2Ge2 (R=La, Ce, Pr, Nd) and Sm2Fe17N3, was determined applying stereologic method of Bodenberger and Hubert. Magnetic domain structure was observed using the powder pattern method (ferrofluid). The domain structure observed is typical for materials with one easy direction of magnetization. The values of domain wall energy density were compared with literature data determined using other methods and a good agreement was stated.
EN
In the paper results of test of wood creep was presented. Creep function of wood at pure bending was also determined.
16
Content available remote Termomechaniczny opis procesu pełzania drewna
EN
In the article the model of wood creep is introduced. The wood consists of cellulose mainly, therefore he is treated as the polymer. In the process The various types of relaxations change in polymers are taken into account in the process.
17
Content available remote Wyznaczanie parametrów funkcji pełzania drewna w ujęciu losowym
EN
In the paper coefficients of creep function of wood at pure bending was determined. They were determined on the basis of measurements of beam deflections. Creep function is time function and beam deflections in following times are random variables. Therefore, analysed problem as stochastic case was treated.
EN
Two series of Prlo+xFe9o-x (x=0; 0.5; 1; 1.5; 2; 2.5; 3; 3.5; 4 and 5 at. %) alloys produced by long time annealing and melt-spinning were investigated. The effects of processing method and alloy composition on the phase structure were determined and compared for these two types of samples using X-ray diffractometry, Mossbauer spectroscopy and transmission electron microscopy. The temperature dependences of magnetization allowed to refine the range of homogeneity region identified for long time annealed samples. Additionally, the magnetic entropy changes ASM were calculated from magnetization measurements performed for Pr^Fes? long time annealed alloy at various temperatures ranging from 266 K to 300K.
PL
W pracy badano dwie serie stopów Pri0+xFe9o-x (x=0; 0,5; 1; 1,5; 2; 2,5; 3; 3,5; 4 and 5 % at.) wytworzonych poprzez długotrwałe wygrzewanie oraz szybkie chłodzenie cieczy na wirującym miedzianym bębnie. Przy użyciu analizy rentgenowskiej, spektroskopii mossbauerowskiej oraz transmisyjnej mikroskopii elektronowej określono i porównano wpływ metody wytwarzania i składu stopu na jego strukturę fazową. W stopach długotrwale wygrzewanych stwierdzono występowanie przedziału stężeń składników, w którym stop jest jednofazowy. Zakres jednofazowości uściślono dzięki badaniom zależności namagnesowania stopów od temperatury. Dla długotrwale wygrzewanego stopu Pr^Fegv określono również zmiany entropii magnetycznej ASM, będące miarą zjawiska magnetokalorycznego.
EN
The microstructure and magnetic properties of bulk glassy Fe6i-xCo7+xZrioMo5W2Bi5 (where x=0, 2, 4) alloy samples in the form of suction-cast rods and tubes and melt-spun ribbons, were investigated. Para- to ferromagnetic ordering transition was observed with increasing Co contents, so that the x=0 alloy was paramagnetic, while the x=4 alloy demonstrated ferromagnetic ordering at room temperature. Analysis of Móssbauer spectra for the amorphous rod, tube and ribbon samples allowed the determination of hyperfine parameters for the amorphous phase. This confirmed paramagnetic ordering of the x=0 alloy amorphous samples. Further analysis of spectra, revealed two non-equivalent surroundings for Fe atoms in the amorphous microstructure, similar to those observed for Fe6oCo8ZrioMo5W2Bi5 rod samples. Similar analysis carried out on amorphous ribbon and rod samples of the x=4 alloy shoved ferromagnetic ordering. The hyperfine field Bhf distributions calculated from the Móssbauer spectra, also indicated non-equivalent surroundings for the Fe atoms. Furthermore, different Bhf distributions were observed for samples produced by various rapid solidification methods. Differential thermal analysis (DTA) revealed a multi-stage crystallization process that is broadly consistent with the Fe sites resolved from the Móssbauer fitting.
PL
W pracy przedstawiono badania mikrostruktury oraz właściwości magnetycznych masywnych stopów amorficznych o składzie: Fe6i-xCo7+xZrioMo5W2B15 (gdzie x=0, 2, 4) wytwarzanych poprzez zasysanie roztopionych łukowo stopów do miedzianej formy chłodzonej wodą oraz jednokierunkowe szybkie chłodzenie na wirującym miedzianym bębnie. Wraz ze wzrostem zawartości Co w składzie stopu obserwuje się znaczny wzrost wartości temperatury Curie próbek amorficznych. Szkła metaliczne stopu zawierającego 7% at. Co wykazują właściwości paramagnetyczne, zaś amorficzny stop zawierający 11% at. Co jest ferromagnetykiem w temperaturze otoczenia. Analiza widm móssbauerowskich prowadzona dla prętów, rurek oraz taśm, pozwoliła na określenie parametrów nadsubtelnych widm odpowiadających różnym otoczeniom atomów żelaza w fazie amorficznej. Badania mossbauerowskie potwierdziły istnienie paramagnetycznego uporządkowania dla próbek amorficznych stopu Fe6iCo7Zr,oMo5W2B15. Dalsza analiza tych widm wykazała istnienie dwu nierównoważnych pozycji atomów żelaza w mikrostrukturze amorficznej, podobnych do obserwowanych w amorficznych prętach stopu Fe6oCo8Zri0Mo5W2B|5. Analiza widm móssbauerowskich amorficznych taśm i prętów stopu Fe57CoiiZrioMo5W2B|5 wykazała istnienie uporządkowania ferromagnetycznego w badanych próbkach. Rozkłady pól nadsubtelnych na jądrach żelaza Bhf, obliczone dla poszczególnych widm móssbauerowskich również w tym przypadku wskazują na istnienie nierównoważnych pozycji atomów żelaza w strukturze amorficznej. Ponadto dla próbek ferromagnetycznych stopu Fe57CoiiZrioMo5W2Bis obserwuje się zmianę rozkładu pól nadsubtelnych w zależności od zastosowanej metody szybkiego chłodzenia. Analiza krzywych DTA wykazała wielostopniowy proces krystalizacji, który można powiązać z istnieniem różnych otoczeń atomów Fe w fazie amorficznej uzyskanych z badań móssbauerowskich.
PL
W pracy analizuje się stan naprężeń i odkształceń w materiale kapilarno-porowatym z mikrouszkodzeniami. Zakłada się, że ośrodek składa się ze składników objętościowych oraz powierzchniowych na granicy faz. W filmie cieczy na powierzchni międzyfazowej uwzględnia się występowanie ciśnień rozklinowujących, które w prezentowanym modelu mają wpływ na uplastycznienie się szkieletu ciała. Finalnie, na podstawie analizy termomechanicznej zostały sformułowane równania konstytutywne sprężysto-plastyczności dla analizowanego ośrodka.
EN
In this paper state of stress and strain in a capillar-porous body with microdamage is analysed. Considered medium consists of volumetric and superficial components. One takes into consideration that disjoining pressure occuring on the interfacial surfaces, has on impact on plasticization of bodys's skeleton. Finally, constitutive equations of elastoplasticity are formulated for the steted problemon the basis of the thermomechanics analisis.
first rewind previous Strona / 2 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.