Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 7

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  dimensional deviation
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
EN
The presented research aimed to obtain information on the effect of cutting parameters and tool wear on the quality of shaped holes in stainless steel package sheets. The testing was planned to allow evaluation of the impact of drilling technology. For this reason, verification tests were performed on a monolithic sheet of the same material grade and thickness equal to the package of four base sheets. It was noted that the double-insert drill is not qualified for use in this process, as it does not provide adequate hole quality (even 0.7 mm deviation in measured diameter from nominal value) and does not provide the expected tool life. Significantly better results were obtained for the monolithic and indexable head drills (IT8). In addition, it was observed that the burr formed when the drill exits the hole, in the case of the indexable double-insert drill, is also significantly larger (~1mm) than for the other tools (less than 0.1 mm). Preliminary tests carried out in this way made it possible to select the tool with the best cutting capability and quality of the generated holes. It was decided to use a drill with an interchangeable head. Tests have shown that it is possible to produce up to 1,000 holes with a diameter of 18.5 mm in a sheet package of 316Ti material with a thickness of 40 mm while maintaining the assumed effective speed of the process (n=1200 rpm, fn=0.18 mm/rev). In experimental testing, a significant effect of cutting speed on tool wear was noted. A correlation between coolant concentration and tool life was also identified - raising the concentration from 8% to 12% increased tool life by virtually 100%. Testing of hole roughness over a full tool life cycle showed that a drill bit with a completed break-in phase provides better hole roughness than a new drill bit. Measuring equipment and software were used for the research and processing of the results – Wenzel XO55, Hommel Etamic LV 17, WM Quartis R2021-1, Grapher 18.3.400, Autodsk Inventor Professional 2023.
PL
Realne powłoki stalowe mają odchyłki od idealnego kształtu, które powstają przede wszystkim na etapie procesu spawania arkuszy blach. Dotychczasowe obserwacje i pomiary stalowych cylindrycznych powłok rzeczywistych pozwoliły na stworzenie modelu spawalniczej imperfekcji reprezentatywnej. Odchyłki od idealnej geometrii cylindrycznej powłoki w postaci promieniowych lokalnych wgłębień mierzone są w praktyce za pomocą przymiarów geometrycznych, których długość jest określona w wytycznych literaturowych i normowych. W pracy wykazano, że istniejące normowe oraz literaturowe zasady oceny klasy jakości wykonania powłok i wynikające z takich ocen wartości nośności wyboczeniowych mogą w wielu przypadkach dawać znacznie zaniżone wartości w stosunku do realnych nośności, wyznaczonych na podstawie indywidualnych analiz GMNIA.
EN
Fabricated steel shells contain deviations from the ideal shape, which arise primarily during the sheet welding process. Previous observations and measurements of real steel cylindrical shells have made it possible to create a model of representative welding imperfection. Deviations from the ideal geometry of a cylindrical shell in the form of radial local indentations are measured in practice using geometric gauges, the length of which is specified in literature and standard guidelines. It was shown in this paper that the existing standard and literature principles of shells fabrication quality class evaluation and the resulting buckling load values may in many cases give significantly lower values in relation to the real load capacity, determined on the basis of individual GMNIA analyses.
PL
Przedstawiono wybrane przykłady imperfekcji geometrycznych, materiałowych i projektowych dotyczących wykonania i montażu prefabrykatów wielkowymiarowych. Podano normowe dopuszczalne wartości odchyłek wymiarów i montażu prefabrykatów.
EN
The article presents selected examples of geometrical, material and design imperfections of manufacturing and assembly of large size precast concrete elements. Limit values of dimensional deviations and assembly of precast elements specified in technical standards are given.
PL
Przedstawiono wyniki badań i analiz statystycznych cech mechanicznych kształtowników i blach walcowanych na gorąco, wyprodukowanych w krajowych hutach w latach 2005-2010. Zestawienie próby statystycznej wytrzymałości współczesnych wyrobów hutniczych jest uzasadnione koniecznością weryfikacji współczynników nośności plastycznej i nośności na rozerwanie – uwzględnianych w ocenie niezawodności konstrukcji stalowych według PN-EN 1993. Ponadto zestawiono próbę statystyczną odchyłek wymiarowych kształtowników walcowanych w badanym okresie oraz przeprowadzono analizę statystyczną geometrycznych charakterystyk dwuteowników walcowanych.
EN
The article presents results of research and statistical analysis of mechanical properties of sheets and hot-rolled sections produced in the domestic steel mills in the years 2005-2010. Elaboration of statistical sample of modern steel products strength is justified by the need to verify factors of yield strength and strength in tension – taken into account in reliability assessment of steel structures according to Eurocode PN-EN 1993. Statistical sample of cross-section dimensions deviations were presented in the article. Statistical analysis of double T-shape geometrical characteristics were performed on the base of collected cross-section dimensions for sections produced in the considered period.
EN
The great number of factors generate situations that real dimensions of each machine elements are different from nominal ones. In the case of rolling bearings elements mentioned disagreements are small – their values are rank of micrometers. However, such small differences can generate significant changes of operational features of bearings. The analysis of influence of ball dimensional deviation on load distribution in ball bearings is presented in this paper. The probability of occurrence of ball diameters of the range of acceptable values is statistically determined. Random distribution of this important dimensions results in other than nominal level of internal stresses (in the contact area of balls and raceways) and therefore true values of some operational features of bearings are other – the most often smaller – than calculated ones. In presented analysis sequence of occurrence of different ball diameters is also taken into account.