The integration of nanomaterials and industrial waste into electromagnetic interference (EMI) shielding composites represents a promising pathway towards sustainable and efficient solutions for modern infrastructure challenges. This paper discusses how these materials are improving, focusing on the nanoparticles and recycled industrial waste that enable them to improve the EMI shielding. Furthermore, the critical applications of EMI shielding composites such as telecommunications, defense, and electronics are elaborated. The mechanical and microstructure properties of cement concrete and mortar based EMI composites are explained in detail. The paper also examines the challenges of producing these materials on a bigger scale and at a reduced cost, as well as the possibilities for future developments. Eventually, this work contributes to the development of high-performing EMI composites that is developed using ecologically friendly materials by minimizing waste which supports sustainable construction.
2
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Przedstawiono dwa rozwiązania termicznego unieszkodliwiania odpadów, czyli procesy zgazowania i pirolizy, wraz z powstającymi w tych procesach produktami ubocznymi, które zawierają części niebezpieczne zarówno dla zdrowia człowieka, jak i dla środowiska, co w niektórych przypadkach uniemożliwia ich dalsze gospodarcze wykorzystanie. Przedstawiono możliwości zastosowania technologii zgazowania i pirolizy w termicznej utylizacji odpadów komunalnych RDF oraz wybranych odpadów przemysłowych. Opisane rozwiązania pokazują, że procesy zgazowania i pirolizy z powodzeniem mogą spełniać wymagania stawiane instalacjom termicznej utylizacji odpadów zarówno komunalnych, jak i przemysłowych. Wymagają one jednak dalszych prac badawczo-rozwojowych, aby mogły być stosowane na szerszą skalę, niż ma to miejsce obecnie.
EN
Methods of thermal disposal of waste using gasification and pyrolysis processes were discussed, along with examples of applications of the by-products generated in these processes. The use of reactors of various designs for thermal waste disposal was discussed. Examples of existing thermal waste disposal plants producing gases used to generate heat/energy were presented.
W artykule zostaną przedstawione prawnośrodowiskowe aspekty zagospodarowania wybranych materiałów odpadowych i ich wykorzystania jako składnika materiałów budowlanych. Jako przykład zostanie przestawione wtórne wykorzystanie materiałów termoplastycznych ze strumienia odpadów komunalnych lub przemysłowych. Część z tych odpadów była poddawana procesom uzdatniania i jest stosowana jako paliwo alternatywne. W proponowanym rozwiązaniu tworzywa termoplastyczne wykorzystuje się jako spoiwo do różnego rodzaju kruszyw. W wyniku formowania takich mieszanek można otrzymywać elementy infrastruktury budowlanej w postaci kostek brukowych, płytek chodnikowych itp.
EN
The article presents legal and environmental aspects of the management of selected waste materials and their use as a component of building materials. As an example, the secondary use of thermoplastic materials from the municipal or industrial waste stream will be presented. Some of this waste was subjected to treatment processes and was used as an alternative fuel. In the proposed solution, thermoplastics are used as a binder for various types of aggregates. As a result of forming such mixtures, elements of construction infrastructure can be obtained in the form of paving stones, paving tiles, etc.
Since the natural raw materials used in the manufacture of clay-based ceramic products vary greatly in the sintering stage, the resulting products are quite heterogeneous. In addition, different types of waste could be used to make ceramic tiles and bricks. Therefore, this study aimed to investigate the effects of pumice, bauxite, and ferrochrome slag on the vitrified ceramic body. In this context, firstly, binary slip mixtures were prepared by composing 40% clay with 60% pumice, bauxite, and ferrochrome slag one by one, which was reduced to 150 μm in particle size. Then, the mixtures were shaped by slip casting method and sintered at 1000°C, 1100°C, 1200°C, and 1250°C. The qualitative XRD analysis was performed in order to see the phase variation, and physical properties were determined with shrinkage and water adsorption measurements. Since pumice transformed into a glassy phase after sintering at 1100°C, an amorphous phase was observed in all samples produced with pumice. In addition, the mullite development occurred in clay-pumice body composition with the temperature increment. However, tridymite and cristobalite phases were analysed in clay bauxite and ferrochrome body compositions. The shrinkage and water adsorption values, which were high in the samples sintered at 1000°C, began to reduce from 1100°C to 1250°C significantly. In particular, water adsorption reached 0% in the clay-pumice system which was suitable for a fully vitrified-high density standard (ISO13006-10545/98). Besides, the brighter colour was reached in the clay-pumice system while brown and black colour was seen in clay-bauxite and clay-ferrochrome bodies, respectively.
Electro-Fenton process could remove pollutant in in tannery industry wastewater. The objectives of this is used to know the effect of electro-Fenton on, ammonia (NH3), chromium (III) (Cr(III), total suspended solid (TSS), biological oxygen demand (BOD), and chemical oxygen demand (COD) removal in tannery wastewater treatment. The voltage variation used to trigger the electro-Fenton reaction was 6 V, 8 V, and 10 V. Observation time at 0, 30, 60, 90, and 120 mins was used to see changes in the sample. The results obtained are electro-Fenton method has an effective time of 30 mins to removal efficiency of 60.7%, 32.9%, 72.8%, 53.4%, and 53.4% for NH3, Cr(III), TSS, BOD, and COD respectively. Pollution from tannery effluent can be eliminated to a sufficient extent using the electro-Fenton technique.
In the work there were presented results of investigations of physico-water properties and water retention ability of chosen post industrial waste in the aspect of natural management. Soil water characteristic curves were determined in pressure chambers with porous ceramic plate and parametrized to the van Genuchten equation. The obtained results show, that the less advantageous retention ability has flotation waste and coal mud, the medium one metallurgical and soda waste. The best retention properties have energetic and heat energetic waste. The determined soil water characteristic curves can be the base for evaluation possibilities of natural management of the investigated waste. The carried out investigations, supplemented by examination of chemical properties enable to choose optimal methods of biological reclamation of landfills where are deposited.
The article concerns the production of lightweight geopolymer concretes based on raw materials from alkali-activated waste, which is consistent with the doctrine of sustainable construction. Fly ash, which is the main component of these geopolymer composites, constitutes energy waste and causes lower emissions of greenhouse gases and other pollutants than traditional cement. The article presents the optimisation of the geopolymer concrete recipe with different dosages of fly ash (200, 300, 400, 500, 600 and 700 kg/m3) and two recipes, the first of which is based on the use of fly ash aggregate, the largest fraction of which was subjected to surface impregnation, and the second one is based on the use of aggregate without any impregnation. Both recipes use an alkaline solution for alkaline activation with a concentration of 6 mol/dm3. Compressive strength tests and apparent density were carried out on the samples. The adequacy of the use of surface impregnation has been demonstrated in the case of low fly ash content (<500 kg/m3), and the optimal recipe based on fly ash in the amount of 600 kg/m3 was indicated.
PL
Artykuł dotyczy wykonania lekkich betonów geopolimerowych na bazie surowców odpadowych aktywowanych alkalicznie wpisujących się w doktrynę budownictwa zrównoważonego. Popiół lotny stanowiący główny składnik danych kompozytów geopolimerowych stanowi odpad energetyczny i powoduje niższą emisję gazów cieplarnianych i innych zanieczyszczeń niż tradycyjny cement. W artykule przedstawiono optymalizację receptury betonów geopolimerowych przy zróżnicowanym dozowaniu popiołu lotnego (200, 300, 400, 500, 600 i 700 kg/m3oraz dwóch receptur, z których pierwsza bazuje na wykorzystaniu kruszywa popiołoporytowego, którego największa frakcja została poddana impreganacji powierzchniowej, a druga bazuje na wykorzystaniu kryszywa bez danej impregancji. W obu recepturach do aktywacji alkalicznej wykorzystano roztwór alkaliczny o stężeniu 6 mol/dm3. Na próbkach przeprowadzono badanie wytrzymałości na ściskanie i gęstości pozornej. Wykazano adekwatność stosowania impregnacji powierzchniowej w przypadku małej zawartości popiołu lotnego (<500 kg/m3) oraz wskazano optymalną recepturę bazującą na popiele lotnym w ilości 600 kg/m3.
This paper presents the results of a composite consisting mainly of industrial waste bound by a hydraulic binder. The composite consists of unburnt coal-mining slate, shredded rubber waste (SRW), fly ash and CEM I cement. The purpose of using the above components was to protect the unburnt coal-mining slate from the negative effects of water, which causes degradation of the aggregate grain size and significantly affects the load-bearing capacity of the aggregate. This was achieved through the use of a binder consisting of shredded waste rubber, fly ash and cement, which imparts hydrophobic properties to the composite. The composite is to be used in road pavement construction and earthworks as a substitute for standard materials. This paper focuses on testing the effects of 5, 10 and 15% additions of shredded rubber waste (SRW) on the physical and mechanical parameters of the composite, mainly compressive strength, water absorption by mass, capillary rise and deformability under cyclic loading. The composite was tested under cyclic loading conditions using a measurement system based on digital image correlation (DIC), with which the deformations occurring on the surface of the test specimens were determined. The results obtained showed the influence of shredded rubber waste additives on the decrease in compression strength (after 7 and 28 days of specimen care), mass water absorption and capillary rise, as well as an increase in the deformability of the composite under destructive loading and cyclic loading.
PL
W pracy przedstawiono wyniki badań kompozytu składającego się głównie z odpadów przemysłowych, związanych spoiwem hydraulicznym. W skład mieszanki wchodzą: łupek przywęglowy nieprzepalony, rozdrobnione odpady gumowe, popiół lotny oraz cement CEM I. Celem zastosowania powyższych składników było zabezpieczenie łupka przywęglowego nieprzepalonego przed negatywnym wpływem wody, który powoduje degradację uziarnienia kruszywa, co znacząco wpływa na nośność kruszywa. Osiągnięto to poprzez zastosowanie spoiwa składającego się z rozdrobnionych odpadów gumowych popiołu lotnego oraz cementu, które powoduje nadanie kompozytowi właściwości hydrofobowych. Mieszanka może być wykorzystana w konstrukcji nawierzchni drogowej oraz w robotach ziemnych, jako substytut standardowo wykorzystywanych materiałów. W artykule skupiono się na badaniach wpływu 5, 10 oraz 15% dodatków rozdrobnionych odpadów gumowych na parametry fizykomechaniczne kompozytu, głównie wytrzymałość na ściskanie, nasiąkliwość masową, podciąganie kapilarne wody oraz odkształcalność pod wpływem cyklicznego obciążenia. W ramach testów kompozytu w warunkach cyklicznego obciążenia został wykorzystany system pomiarowy opierający się na cyfrowej korelacji obrazu (DIC), za pomocą którego określono odkształcenia zachodzące na powierzchni badanych próbek. Uzyskane wyniki badań pozwoliły stwierdzić wpływ dodatków rozdrobnionych odpadów gumowych na zmniejszenie się wytrzymałości na ściskanie (po 7 oraz 28 dniach pielęgnacji próbek), nasiąkliwości masowej i wysokości podciągania kapilarnego oraz podwyższenie odkształcalności kompozytu pod wpływem obciążeń niszczących, jak i obciążenia cyklicznego. Zaprezentowany kompozyt ze względu na swój skład, w którym wykorzystuje się głównie odpady przemysłowe dobrze wpisuje się w gospodarkę o obiegu zamkniętym oraz pozwala na znalezienie nowego sposobu wykorzystania odpadów górniczych, których utylizacja ciągle stanowi problem w Zagłębiu Górnośląskim.
9
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
W pracy przedstawiono wyniki badań dotyczące kinetyki uwalniania metali ciężkich (cynk, miedź i ołów) z próbek żużla stalowniczego stanowiącego uboczny produkt procesu wytapiana stali oraz mułu powstałego z mokrego oczyszczania spalin w spalarni śmieci. Analizie poddano materiał pobrany w trakcie wyjazdu technologicznego na terenie Zakładu Odzysku Surowców Madrohut Sp. z o.o. w Krakowie. W pracy przedstawiono charakterystykę próbek, sposób przygotowania ich do badań oraz procedurę analityczną. Ocenę ilości uwalnianych do roztworu metali ciężkich przeprowadzono w oparciu o pomiary woltamperometryczne z wykorzystaniem techniki impulsowej różnicowej DPV (ang. Differential Pulse Voltammetry) oraz elektrody rtęciowej o kontrolowanym wzroście kropli jako elektrody pracującej. Wyniki badań wskazują, że spośród badanych metali, cynk jest metalem, który uwalnia się w największym stopniu, około 25 razy więcej w stosunku do miedzi oraz około 40 razy więcej w stosunku do ołowiu. Analiza otrzymanych wyników wykazała, że największa ilość badanych metali uwalnia się w czasie pierwszej godziny. Ponadto, dłuższy czas wymywania nie powodował wzrostu stężenia cynku, ołowiu oraz miedzi w wymywanym roztworze.
EN
This paper presents the results of a study on the kinetics of heavy metal (zinc, copper and lead) release from samples of steelmaking slag, which is a by-product of the steel smelting process, and sludge generated from wet flue gas treatment at a waste incinerator. The material was analyzed during a process trip at the site of the Madrohut Raw Materials Recovery Plant Ltd. in Krakow. The paper presents the characteristics of the samples, their preparation for testing and the analytical procedure. Evaluation of the amount of heavy metals released into solution was carried out based on voltammetric measurements using Differential Pulse Voltammetry (DPV) and a mercury electrode with controlled droplet growth as the working electrode . The results show that of the metals tested, zinc is the metal that releases the most, about 25 times more than copper and about 40 times more than lead. Analysis of the results obtained showed that the largest amount of the metals tested is released during the first hour. In addition, a longer leaching time did not increase the concentration of zinc, lead and copper in the leached solution.
In this paper, the finite element method (FEM) is applied to calculate the bearing capacity of two footings having the aspect ratio L/B (where L and B are the length and width of the footing, respectively) equal to 1, 2 resting on one-layer and two-layer soil. Soil profile contains two soil types including sand and clay. The soil strip is 500mm × 500mm × 350mm; however, only a quarter of the model (250mm × 250mm × 350mm) is examined in the study. Two primary situations are investigated in this study. In the first situation, the one-layer system is supposed to be sandy soil with footing overlays on medium-dense sand. The soft clay/stabilized clayey layer is supposed to be on top of the sandy soil in the second condition, with the footing resting on top of the soft clay/stabilized clay. The influence of layer thickness, aspect ratio, and material property on the bearing capacity value and footing failure mechanism is studied for eight different combinations of layered soil. The bearing capacity for a one-layer case is also estimated, and it agrees well with Vesic (1973), Hansen (1970), and Terzaghi's (1943) equations. The bearing capacity of footings is observed to decline when the height of unstabilized clayey soil increases, and it increases when clayey soil is stabilized with molasses, waste foundry sand, and lime alone and in combination with each other.
The article reviews the current state of the art in the field of zinc recycling. The results of model studies of the profitability (profitability) of the process of zinc recovery in precipitation in the form of dusts and sludges are presented. The cost of purchasing waste and the necessary energy and material expenditures were taken into account. It has been shown that access to a cheap source of waste is essential for the profitability of the zinc recovery process.
Drogownictwo oraz jego część związana z robotami ziemnymi charakteryzują się bardzo dużym zapotrzebowaniem na naturalne materiały budowlane, takie jak grunty oraz kruszywa. Powoduje to, iż mimo bardzo dużych pokładów tych zasobów ich ilość bardzo szybko się kurczy. Odpowiedzią na ten problem powinno być wykorzystanie odpadów przemysłowych jako materiału budowlanego. Idea ta bardzo dobrze wpisuje się w coraz popularniejszy system ekonomiczny gospodarki o obiegu zamkniętym, gdzie produkty uboczne procesów technologicznych pochodzących z jednej gałęzi przemysłu służą jako surowce produkcyjne w innych gałęziach przemysłu. W artykule przedstawiono propozycję takiego materiału budowlanego składającego się z trzech odpadów przemysłowych związanych spoiwem hydraulicznym. Sktadnikami kompozytu są łupek przywęglowy nieprzepalony (Ł) rozdrobnione odpady gumowe (G), popiół lotny (P) oraz cement CEM I 42,5 (C). Mieszance nadano roboczą nazwę ŁGPC. Celem jej wytworzenia była możliwość zagospodarowania jak największej ilości odpadów przemysłowych, z wykorzystaniem rozdrobnionych odpadów gumowych (ROG) do zabezpieczenia łupka przywęglowego nieprzepalonego przed szkodliwym działaniem wody. Zastosowanie rozdrobnionych odpadów gumowych ROG, a dokładniej spoiwa gumowo-popiołowo-cementowego (GPC), powoduje nadanie mieszance pewnych właściwości hydrofobowych. Woda oddziałująca na łupek przywęglowy wywołuje degradację jego uziarnienia (rozpad większych ziaren kruszywa), co prowadzi do spadku jego nośności oraz do możliwości uzyskania właściwości wysadzinowych. W pracy przedstawiono wyniki badań nad wpływem zawartości ROG (dodatki 5, 10 oraz 15%) na wartości wytrzymałości na ściskanie, nasiąkliwości masowej oraz wysokości podciągania kapilarnego wody przez próbki wykonane z kompozytu. Dodatkowo na podstawie dotychczasowych wyników badań przedstawiono możliwości zastosowania kompozytu w warstwach konstrukcji nawierzchni drogowej, zgodnie z wytycznymi dotyczącymi warstw konstrukcji nawierzchni drogowej związanych spoiwem, zawartymi w Wytycznych technicznych nr 5 oraz w wytycznych francuskich.
EN
Road construction and its part related to earthworks are characterized by a very high demand for natural building materials such as soils and aggregates. As a result, despite the very large deposits of these resources, their quantity is shrinking very quickly. The answer to this problem should be the use of industrial waste as a building material, an idea that fits very well into the increasingly popular Closed Circuit Economy economic system, where by-products of technological processes from one industry are used as production raw materials in other industries. The article presents a proposal for such a building material consisting of three industrial wastes bound by a hydraulic binder. The components of the composite are unburned coal slate (S), shredded rubber waste (R), fly ash (F) and CEM I 42.5 cement (C), the mixture was given the working name SRFC. The purpose of its manufacture was to be able to manage as much industrial waste as possible, using shredded rubber waste (SRW) to protect unburned coal shale from the harmful effects of water. The use of shredded rubber waste SRW and, more specifically, a rubber-ash-cement binder (RFC) results in giving the mixture certain hydrophobic properties. Water interacting with the coal slate causes degradation of its grain size (disintegration of larger aggregate grains), which results in a decrease in its load-bearing capacity and the possibility of obtaining blow-out properties. This paper presents the results of a study on the effect of SRW content (additives of 5, 10 and 15%) on the values of compressive strength, bulk water absorption and the height of capillary rise of water by samples made of the composite. In addition, on the basis of previous research results, the possibility of using the composite in road pavement construction layers is presented, based on the guidelines for binder-bonded road pavement construction layers contained in Technical Guideline No. 5 and French guidelines.
The focal theme of this study is to evaluate the life cycle of asphalt mix containing Jordanian oil shale ash (OSA). Life cycle assessment (LCA) approach was conducted to assess the environmental impact of all manufacturing stages of the asphalt mix from Global warming potential (GWP) and energy consumption (EC) perspectives. The documentation for the LCA study was done in accordance with ISO 14044:2006 standards for the research’s goal and scope, inventory analysis, impact assessment, and interpretation. The results revealed that replacing the asphalt mix partially with Jordanian OSA (10 wt.%) resulted in slight reduction in both GWP and EC. A reduction of 2.83% and 4.8% for GWP and EC, respectively, was obtained.
The article deals with the studies on complex sorption treatment of industrial waste of various industries to obtain new C, S, N-containing plastic lubricants, which provide antiwear, antifriction, high load-bearing and heat-resistant properties. The conditions for obtaining diethylammonium salt from the obsolete pesticide Banvel D and its sorption on a mixed sorbent, which consist of activated carbon (AC) and kieselguhr (K), have been established. The conditions for obtaining potassium diethyldithiocarbamate and its adsorption on the surface of the mixed sorbent (AC + K), followed by treatment with copper(II) sulfate of corresponding bis-(diethyldithiocarbamato)copper(II) sorbed on a solid surface, have been examined. The obtained substances of general composition [sorbent (AC + K)]·[(C2H5 )2NS(=S)S]2Cu were studied as active components of plastic lubricants, which provide their thickening, antiwear and antifriction properties. Industrial tribological research was carried out for friction pairs of four-row roller bearings of roller equipment used at private enterprise (PE) "Exim" (Kherson, Ukraine).
Since organic dyes are the main component of many industrial wastes, it is necessary to be removed efficiently and instantaneously. The aim of this research focuses on the synthesizing of organoclay by modifying kaolinite with cetyl trimethyl ammonium bromide and applying it for the removal of (methyl-orange) dye from water by the mechanisms of adsorption. The effects of several parameters, mainly agitation time, water pH, adsorbent doses, and dye concentrations, on the adsorption process were optimised using the central composite design (CCD) method, which was performed using MINITAB package (version 17). Results showed that the dye was completely (100%) removed at pH of 4.0, adsorbent dose of 0.4 g, dye concentration of 50 mg/L, and agitation speed of 160 rpm. In addition, it was found that Freundlich and Sips isotherms were the best models to track lab data. Moreover, the Pseudo second order method was found to be more convenient compared to other models for studying kinetics of the sorption mechanism. For column testing, an appropriate hydraulic conductivity and reactivity were obtained by combining modificatory kaolinite and glass waste with weight proportions of 50:50. Thus, empirical simulations such as those in the kinetic model of Clark have provided satisfactory consent for using the simulated methyl orange.
16
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Polska jest drugim producentem sody kalcynowanej w Europie. Roczna produkcja sody w naszym kraju szacowana jest na 1,2 mln ton. Stosowany do produkcji sody proces Solvay’a generuje znaczne ilości współproduktów, które w zależności od składu i właściwości mogą mieć charakter produktu ubocznego lub odpadu, stanowiąc istotny problem zakładów produkujących sodę. Należy do nich tzw. wapno posodowe, które w praktyce powstaje na kilku etapach produkcji sody, różniąc się w sposób istotny składem i właściwościami. W konsekwencji opis składu i właściwości takiego materiału, z pominięciem dokładnego źródła powstania w procesie technologicznym, jest często niejednoznaczny. Prowadząc badania nad wapnem posodowym konieczne jest zatem zróżnicowane podejście do różnych frakcji wapna posodowego jako odmiennych, niezależnych materiałów.
EN
Poland is the second producer of soda ash in Europe. The annual production of soda in Poland is estimated at 1.2 million tonnes. However, the Solvay process used for the production of soda ash generates significant amounts of co-products, which, depending on the composition and properties, may be a by-product or waste, constituting a significant problem for soda production plants. They include the so-called "post-soda lime", which in practice is formed at several stages of soda production, differing significantly in composition and properties. As a consequence, the description of the composition and properties of such material, omitting the exact source of its formation in the technological process, is often ambiguous. When conducting research on post-soda lime, it is, therefore, necessary to have a differentiated approach to different fractions of post-soda lime as separate, independent materials. This study is a review of knowledge on the formation, properties, and possibilities of using post-soda lime from the production of soda ash using the Sovaya method. Keywords: postsoda lime, circular economy, neutralization of fluorides, industrial waste, sorbents.
This study provides a comparative analysis of natural nanosilica (NSn), which is an extract of natural silica sand processed into nanosilica with commercial nanosilica (NSc) derived from semiconductor industrial waste, in 80 MPa high performance concrete (HPC). The percentage of using nanosilica is (3%, 5%, 10%, 15%) by weight of cement used directly and combined with 5% silica fume. Analysis was carried out through compressive strength test, durability through permeability test, rapid chloride penetration test (RCPT), and microstructure test through scanning electron microscopy (SEM). The results of the analysis show that natural nanosilica is equivalent to commercial nanosilica, in applications it is better to use silica fume incorporation. The optimum percentage of using NSn10% and (SF) 5%, while 5% NSc and 5% SF, in these proportions shows the best compressive strength and durability. It’s just that the use of natural nanosilika is 5% more than commercial nanosilika. The benefit of this research is that natural materials such as silica sand with high SiO2 content, can be processed into nanosilica as an advanced material, which can be used as an eco-friendly construction material.
Kontrole w zakresie ochrony środowiska, a zwłaszcza gospodarki odpadami budzą wiele emocji i wątpliwości przedsiębiorców. Przedsiębiorcy często zadają pytania: jakie uprawnienia posiada kontrolujący, czy korzystający z władztwa organ kontrolujący może żądać dokumentów niezwiązanych bezpośrednio z zakresem kontroli, czy i kiedy może dojść do wyłączenia pracownika organu? Jakie są środki ochrony prawnej przeciwko ustaleniom zawartym w protokole kontroli, a także jakie są skutki podpisania protokołu z pokontrolnego? Są to tylko niektóre istotne zagadnienia związane z prowadzoną kontrolą.
19
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Na rekultywowany teren pogórniczy naniesiono substrat glebowy zawierający osady ściekowe. Oznaczono zawartość metali ciężkich w próbkach nowo powstałej gleby pobranej z tego terenu i gleby kontrolnej. Obliczono wskaźnik zanieczyszczenia dla substratu glebowego i Taraxacum officinale metalami ciężkimi na obszarze poeksploatacyjnym. Stwierdzono korzystny wpływ materiału doglebowego na zdegradowane tereny pogórnicze. Odpady przemysłowe i komunalne mogą być wykorzystane w gospodarce o obiegu zamkniętym i rekultywacji terenu.
EN
Sewage sludge mixt. was deposited on the post-mining area. The content of heavy metals in soil samples was taken from both study and control site. The heavy metal contamination index for the soil substrate and Taraxacum officinale in the post-mining area was calculated. The beneficial effect of soil substrate on reclaimed post-mining areas was found. Industrial and municipal waste can be used for a circular economy and land reclamation.
20
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW