The Ni – base superalloys are used in aircraft industry for production of aero engine most stressed parts, as are turbine blades or turbine discs. The most stressing factor at Ni – base superalloys loading or working conditions are high temperature range of 700°C up to 850°C and, of course, centrifugal forces, and small vibrations, which produce bending of turbine blades inserted into turbine discs. All these factors cause various forms of microstructure degradation closely connected with decreasing of mechanical properties and shortening of working life as well. From this reason a dendrite arm spacing, carbides size and distribution, morphology, number and value of γ’ - phase are very important structural characteristics for blade lifetime prediction as well as aero engine its self. In this article are used methods of quantitative metallography for evaluation of structural characteristics mentioned above on experimental materials – Ni base superalloys ŽS6K and Inconel IN 738. The high temperature effect represented here by heat treatment at 800°C for 10 hours, and cooling rate, here represented by three various cooling mediums as water, air, and oil, on structural characteristics and application of quantitative methods evaluation with using of SEM are presented in this paper.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.