This study delves into the influence ofwater film thickness (WFT) on the rheological characteristics, particularly the yield stress, of cement paste incorporating limestone powder. Employing an Anton Paar MCR 102 rheometer, precise measurements of both the static and dynamic yield stress were conducted. Artificial neural networks (ANN) were then applied to explore the relationship between WFT and yield stresses. The findings reveal an approximate linear growth pattern in the shear stress-shear rate profile of cement-limestone paste, with an intensified shear thickening observed as limestone powder content increases. The augmentation of limestone powder and specific surface area notably enhances both static and dynamic yield stresses, with the latter reaching 70.26 Pa in the case of a paste containing 50% Class III limestone powder (1088 m2/kg). The WFT of cement-limestone paste particles is contingent on the ratio of solid particle packing density to total specific surface area, exhibiting an increase with rising solid particle packing density. Both static and dynamic yield stresses exhibit a negative correlation with WFT. Artificial neural networks demonstrate efficacy in predicting static and dynamic yield stresses based on mix ratio parameters and WFT, with a higher prediction accuracy for static yield stress, reflected in an R2 value of 0.9745.
2
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Wykorzystanie dodatków mineralnych do cementu i betonu jako częściowego substytutu cementu jest jednym z najskuteczniejszych sposobów obniżenia emisji dwutlenku węgla w produkcji cementu. Chociaż wcześniejsze badania nad wykorzystaniem popiołu z trzciny cukrowej, wytłoków z trzciny cukrowej [SBA] i wapienia jako częściowego substytutu cementu, zostały opublikowane, to jednak niewiele jest badań na temat ich łącznego zastosowania w cemencie. Wpływ SBA i wapienia na kinetykę hydratacji cementów mieszanych badano poprzez określenie właściwości mieszanek oraz stwardniałych zapraw uzupełnionych analizą TGA i XRD. Połączone efekty aktywności pucolanowej SBA i efektu zarodkowania wapienia w cemencie trójskładnikowym, B15L10 pozwoliły na uzyskanie największej wytrzymałości na ściskanie. Po dodaniu SBA i wapienia wyraźnie zanotowano zmniejszenie zawartości portlandytu w dwuskładnikowych i trójskładnikowych cementach mieszanych przy użyciu XRD i TGA. W zaczynie B15L10 stwierdzono około 44% zmniejszenie zawartości portlandytu w porównaniu z zaczynem kontrolnym. Dodatkowe produkty hydratacji, takie jak hemikarboglinian i monokarboglinian, powstają w wyniku dodania wapienia do mieszanego cementu, co sugeruje synergiczną reakcję między SBA a wapieniem.
EN
The utilization of supplementary cementitious material [SCMs] as a partial substitution of cement is one of the most effective way to lower carbon-dioxide emissions in the cement production. Although previous research on the use of sugarcane bagasse ash [SBA] and limestone as SCMs as a partial substitution of cement has been reported. However, there is little research on their combined use in cement. The impact of SBA and limestone on the hardening and hydration property in blended cements were examined by testing properties of fresh and hardened mortars supplemented with TGA and XRD analysis. The combined effects of SBA pozzolanic reaction and limestone nucleation effect in ternary cement, B15L10 exhibits the maximum compressive strength. With the addition of SBA and limestone, a reduction in portlandite content was clearly observed in binary and ternary blended cements using XRD and TGA. B15L10 accounts for about 44 % decrease in portlandite when compared to control observed by TGA. Additional hydration products like hemicarboaluminate and monocarboaluminate are produced as an outcome of the addition of limestone in blended cement were detected by XRD which implies synergistic reaction between SBA and limestone.
3
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Mineral admixtures and waste by-products in concrete exhibit economical and environmental benefits, but their cementing and engineering properties should be assessed before practical adoption. In this study, we investigated hydration and physical properties of Self-Consolidating (SCM) and Ordinary (OM) mortars, based on slag-blended Portland limestone cement (PLC), with equivalent water-to-cement ratio (E/C≈ 0.55). The variables were mortar type and mineral admixture type, limestone powder (LP) or silica fume (SF). Therefore, we made two ordinary mortars (OMs), Oref (OPC based) and Oplc (slag PLC based), and two self-consolidating mortars (SCMs), SplcL (limestone based) and SplcS (silica fume based). We assessed compressive strength, sorptivity, hydration heat, thermogravimetric analysis, and SEM images. Results reveal that Oplc exhibits similar to better performance than Oref; blended LP leads to 36% higher mechanical strength, more than 50% carboaluminate in SCMs, and 40% lower heat and rate of hydration, and seems to have packing role and doesn't contribute to more sites’ nucleation; SF is efficient when substituted more than 10%.
4
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
W artykule przedstawiono wpływ dodatków pochodzenia odpadowego: zmielonego wapienia i pyłu krzemionkowego na właściwości jednokomponentowej zaprawy uszczelniającej. Stosując te dodatki, redukowano jednocześnie udział cementu CEM I i wypełniaczy kwarcowych. Zbadano wpływ takich modyfikacji na ważne właściwości zapraw uszczelniających: porowatość określaną na powierzchni przełomu próbki metodą mikroskopową; przyczepność do podłoża betonowego oraz wodoszczelność. Stwierdzono negatywny wpływ zmielonego wapienia na wodoszczelność i przyczepność zaprawy do podłoża betonowego oraz poprawę wodoszczelności i zmniejszenie porowatości w wyniku dodatku pyłu krzemionkowego.
EN
In the publication, the effect of addition of a waste product: limestone powder and silica dust on one-component sealing mortar is presented. By adding these components, the share of CEM I cement and quartz fillers was reduced. The impact of these modifications on the important properties of sealing mortars was investigated: porosity determines the fracture surface by microscopic method, approach to the concrete substrate and water tightness. A negative effect of limestone powder on the tested properties and an improvement in water permeability and porosity due to the addition of silica fume was found.
W artykule przedstawiono badania efektów zastosowania w betonie 8 różnych mączek wapiennych, poprzez zastąpienie nimi aktywnego dodatku pucolanowego. Wyniki badań potwierdziły ich przydatność, a ostateczna ocena może nastąpić na podstawie badań wstępnych. Użycie mączek wapiennych bezpośrednio do betonu wpisuje się w działania zmierzające do obniżenia emisyjności tego bardzo ważnego materiału konstrukcyjnego.
EN
The article presents research on the effects of using 8 different limestone powders in concrete by replacing the active pozzolanic additive with them. The results of the research confirmed their suitability, and the final assessment may be based on initial test. The use of lime powder directly into concrete is part of the activities aimed at reducing the emissivity of this very important construction material.
6
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Przedstawiono wyniki badań procesu brykietowania składowanych na zwałowiskach mieszanek wysokowapniowych szlamów pofiltracyjnych o wilgotności 21,28% z wodorotlenkiem wapnia, mączką wapienną lub kredą techniczną w prasie walcowej, wyposażonej w pierścienie o niesymetrycznym układzie zagęszczania zasilanej grawitacyjnie. Wyznaczono wytrzymałość brykietów na zrzut oraz wytrzymałość na ściskanie. Określono najkorzystniejszy z punktu widzenia wytrzymałości mechanicznej brykietów udział masowy poszczególnych dodatków. Ze względu na swoje parametry fizykochemiczne mogą być one zagospodarowane w rolnictwie oraz przemyśle cementowym.
EN
High-calcium filtered sludge with the addn. of hydrated lime or lime-stone powder or fine technical chalk were briquetted in a roller press equipped with asymmetrical thickening layout and gravity feeding. The drop strength and the compressive strength of briquettes were detd. The most advantageous mass fraction of individual additives was detd. from the point of view of the mech. strength of briquettes. They can be used in agriculture and the cement industry.
7
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
W pracy przedstawiono wyniki badań wpływu granulowanego żużla wielkopiecowego, naturalnej pucolany [superzeolit] i mączki wapiennej na właściwości cementów wieloskładnikowych. Stwierdzono, że synergiczne połączenie wymienionych dodatków mineralnych, biorąc pod uwagę wpływ rozkładu wielkości cząstek według objętości i powierzchni, a także ustalenie wskaźników wpływu czynników fizycznych, takich jak wodoządność, wydzielanie mleczka, aktywność pucolanowa, ciepło hydratacji na zestaw właściwości zaczynu i betonu: urabialność, wytrzymałość normowa i wczesna, emisja CO2, pozwala uzyskać technologicznie zoptymalizowane cementy portlandzkie wieloskladnikowe. Wyniki wykazały, że oddzielne mielenie poszczególnych składników, optymalizacja składu ziarnowego żużlia, superzeolitu i mączki wapiennej, z uwzględnieniem rozkładu wielkości cząstek według powierzchni, umożliwia wytwarzanie cementu portlandzkiego wieloskładnikowego o dużej wytrzymałości wczesnej CEM II/B-M 42,5 R LH.
EN
The paper presents the results of research on the influence of granulated blast furnace slag, natural pozzolana [superzeolite], and limestone powder on the performance of multi-component cements. It was found that the synergistic combination of mineral additives of different genesis, taking into account the influence of the particle size distribution [PSD] by volume and surface area, as well as the determination of indicators of the influence of physical factors such as water demand, bleeding, pozzolanic activity, the heat of hydration on the set of properties of paste and concrete: workability, standard, and early strength, global warming potential, allows to obtain technologically optimized multi-component Portland cements. The results showed that the production of multi-component Portland cement with high early strength CEM II/B-M 42.5 R-LH ensures separate grinding of individual constituents, optimization of grain composition of slag, superzeolite, and limestone powder taking into account the PSD by surface area.
8
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Porównano wyniki badań aglomeracji mieszanki wapienno-gipsowej realizowanej w trybie jednoetapowym w granulatorze mieszalnikowym, talerzowym lub bębnowym z efektami granulacji dwuetapowej. Do granulacji użyto mieszanki (w proporcji 1:1) mączki wapiennej i gipsu będącego odpadem z procesu odsiarczania spalin. Proces granulacji prowadzono w sposób okresowy. Każdorazowo, po przeprowadzonym doświadczeniu określano skład granulometryczny uzyskanego produktu oraz jego odporność na ściskanie.
EN
Mixts. of limestone powder and gypsum (1:1 mass ratio) and aq. 20% solns. of molasses added to them in various amts. as a binding liq. were used for (i) one-step or (ii) twostep granulation. Variant (i) included the use of the selected granular type (a mix, disc or drum granulator) while variant (ii) included of a mixer and then the disc or drum granulator. The compressive strength of the granules and their granulometric compn. in the fraction range up the 8 mm were detd. for each variant of the process. An increase in molasses content in mixts. as well as the time of granulation resulted in an increase of the av. size of granules and their compressive strength for all granulation variants.
9
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Przedstawiono wyniki badań okresowej granulacji bębnowej mączki wapiennej pochodzenia jurajskiego przy użyciu wybranych cieczy wiążących, dla różnych parametrów procesowo-aparaturowych. Do nawilżania użyto wodne roztwory trzech cieczy: szkła wodnego, poli(alkoholu winylowego) (PVA) i melasy o różnych stężeniach. Jako zmienne parametry procesowe stosowano iloraz objętości dodanej cieczy wiążącej do masy granulowanego surowca, czas podawania cieczy wiążącej i całkowity czas granulacji. Określono wpływ badanych parametrów na właściwości otrzymanego produktu skład granulometryczny, wytrzymałość granul na ściskanie i szybkość rozpadu cząstek w środowisku wodnym.
EN
Aq. solns. of water glasses, poly(vinyl alc.) and molasses with various concns. were sep. added to the shredded limestone powder (grain diam. 300 μm, CaCO3 93-95%, MgCO3 1.5%) and then subjected to periodic drum granulation for 5-30 min. The effect of binder type, its concns. in aq. soln., amt. of binder in relation to limestone powder as well as granulation time on the compressive strength of granules and on a degree of their decompn. after contact with a aq. environment (30 min) were detd. The increasing concn. of each type of binder and its amt. in relation to limestone powder as well as the time of granulation resulted in an increase of the compressive strength of granules. Granules obtained by using the molasse binder reached the largest compressive strength as well as the highest degradn. degree.
The preliminary stage of asphalt mixture production involves the drying and dedusting of coarse aggregates. The most common types of coarse aggregates used are limestone and basalt. In the process of drying and dedusting the dryer filter accumulates large quantities of waste in the form of mineral powder. This paper introduces an investigation into limestone powder waste as a potential microfiller of polymer composites. Physical characteristics such as the granulation the of powder collected from the filter - in terms of the season of its collection and the type of input materials used - were analysed. A scanning electron microscope (SEM) was used for the investigation described within this paper. The obtained results were compared against those of other materials which can be used as polymer composites microfillers.
PL
Wstępnym etapem produkcji mieszanek mineralno-asfaltowych (MMA) jest suszenie i odpylanie kruszywa grubego. Najczęściej stosowanymi typami kruszyw w produkcji MMA są wapienie i bazalty. W czasie procesu ich wstępnego przygotowania w suszarkach gromadzą się duże ilości odpadu w postaci pyłu mineralnego. Uziarnienie pyłów pochodzących z filtrów suszarek zależy nie tylko od wkładu surowcowego, ale również od pory roku w której pyły zostały zgormadzone. Pyły pochodzące z odpylania kruszyw o podobnym składzie mineralnym wykazują podobne uziarnienie. Znaczące różnice mogą zostać zaobserwowane, gdy porównane zostaną pyły pochodzące z odmiennych wkładów surowcowych. Dalsze analizy były przeprowadzone dla pyłu wapiennego zgromadzonego w maju. Można zauważyć, że pomimo iż charakter uziarnienia pyłu wapiennego jest odmienny od najczęściej stosowanej mikrokrzemionki to wartość najczęstsza jest zbliżona. Uziarnienie odpadowego pyłu wapiennego jest zbliżone do uziarnienia mikrokrzemionki, jednakże odznacza się zwiększoną zawartością grubszych ziaren (średnica 50-100m). Warto jednak zauważyć iż prawie w całości odpad spełnia wymagania stawiane mikrowypełniaczom (98% ziaren ma średnicę poniżej 120 µm).
11
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Strumienie wejściowe (węgiel, mączka kamienia wapiennego, woda procesowa) i wyjściowe (popioły lotne z 3 stref odpylania, żużel, gips, osad i odciek z odsiarczania spalin) zostały poddane analizie elementarnej w celu sporządzenia bilansu materiałowego 58 pierwiastków. Materiały pochodziły z bloku energetycznego wyposażonego w 3-strefowy elektrofiltr i system mokrego odsiarczania gazów spalinowych. Stwierdzono, iż węgiel jest materiałem warunkującym skład ubocznych produktów spalania. W osadzie z odsiarczania spalin były zawarte zwiększone ilości pierwiastków ziem rzadkich, a Ca, S, Ge i Se obecne były w dużym stężeniu w gipsie i osadzie.
EN
Ingoing streams (coal, limestone powder, process H2O) and outgoing streams (fly ashes from three stages of electrostatic precipitator, slag, gypsum, sludge and sewage from desulfurization system) were analyzed for elemental compn. to develop material balances of particular 58 elements. Materials were derived from Polish coal-fired power plant equipped with a 3-stage electrostatic precipitator and wet flue gas desulfurization system. The elemental compn. of coal combustion products mostly depended on the coal compn. The rare earth elements were concd. mainly in the sludge from wet desulfurization, while Ca, S, Ge and Se in the gypsum and in the sludge.
Badano surowe i hydrofobowe pyły wapienne. Proces hydrofobizacji prowadzono za pomocą typowych przemysłowych modyfikatorów: kwasu stearynowego, preparatu silikonowego oraz preparatu bitumicznego. Właściwości hydrofobowe materiałów określano w oparciu o wyniki pomiarów kątów zwilżania, uzyskane metodami: siedzącej kropli, wzniesienia kapilarnego oraz zwilżania cienkiej warstwy. Otrzymane wyniki umożliwiły określenie właściwości powierzchniowych hydrofobowych proszków wapiennych.
EN
Raw and hydrophobized limestone powders were studied. The hydrophobi zation was carried out with the use of typical commercial modifiers: stearic acid, silicone preparation and bituminous preparation. Hydrophobic properties of materials were obtained based on results of wetting angle measurements made by sessile drop, capillary rise and thin layer wicking methods. Obtained results enabled one to determine the surface properties of hydro-phobic limestone powders.
Limestone powder characterized by hydrophobic properties is used as an anti-explosive agent in coal mining industry. Unfortunately, the standard method of producing such powder by milling limestone with stearic acid is practically unprofitable in many modernized quarries and plants, and sometimes literally impossible due to the introduction of technological changes and implementation of modern mills. Then new methods of hydrophobization of limestone surfaces ought be searched. In the work two methods hydrophobization: from the stearic acid vapour phase and from silicone solutions are proposed. Lime dust from the Czatkowice Quarry of Lime was used as a raw material during investigations. It is a good agent for research because it is possible to compare the properties of samples modified in this work to the properties of anti-explosive lime powder (Polish Standard, 1994) used in mining industry in Poland. The first technique of limestone powder hydrophobization was carried out in an apparatus of own design (Vogt, 2008, 2011), and it consisted in free sedimentation of the powder layer dispersed by stearic acid vapour in powder counter current flow. The second way of modification consisted in mixing in the evaporating dish substrates: limestone powder and dope - silicone solution - Sarsil® H-15 (Vogt & Opaliński, 2009; Vogt & Hołownia, 2010). Evaluation of properties so-obtained waterproof powders was carried out according to the Polish Standard, as well as using original powder determination ways, with the Powder Characteristic Tester (Index tables, Tablets & Capsules, 2005). Moreover water vapour adsorption isotherms were obtained and the thermal decomposition of powder was made. All modified samples acquired the hydrophobic character. Therefore we can state that the both proposed methods of hydrophobization of the limestone powder are useful. The parameters obtained with the use of Powder Characteristics Tester enable us to make a characterization of limestone properties not only as a water resistant material but also from the cohesion point of view. On the base of TG, DTG or DTA and EGA curves for all investigated materials was stated that the character of the thermal decomposition of modified samples is the same as this one for raw powder, what is profitable for application of hydrophobized powders as an anti-explosive agent.
PL
W górnictwie węgla kamiennego używany jest hydrofobowy pył wapienny jako substancja stosowana w systemie zabezpieczeń przeciwwybuchowych (Cybulski, 2004). Niestety, dotychczasowy sposób wytwarzania takiego produktu polegający na współmieleniu kamienia wapiennego z kwasem stearynowym staje się praktycznie niemożliwy do stosowania w nowoczesnych zakładach np. kamieniołomy. Sytuacja taka jest wynikiem wprowadzania zmian technologicznych, głównie związanych z wymianą starych konstrukcji młynów na nowe urządzenia. Tym samym istnieje potrzeba poszukiwania nowych metod hydrofobizacji powierzchni pyłów wapiennych. W pracy omówiono dwie nowe metody hydrofobizacji pyłu wapiennego: za pomocą par kwasu stearynowego oraz roztworu silikonowego - Sarsil® H-15. Podczas badań używano surowego pyłu wapiennego pochodzącego z Kopalni Kamienia Wapiennego w Czatkowicach. Materiał ten jest dobrym materiałem do badań gdyż istnieje możliwość porównywania właściwości materiałów hydrofobowych otrzymanych w pracy z właściwościami handlowego pyłu przeciwwybuchowego (Polska Norma, 1994), używanego w polskich kopalniach. Pierwszy sposób hydrofobizacji pyłu wapiennego, polegający na swobodnym opadaniu pyłu wapiennego w oparach kwasu stearynowego przepływających w przeciwprądzie, przeprowadzono w aparacie własnej konstrukcji (Vogt, 2008, 2011). Aparat gwarantuje dobry kontakt modyfikatora z ziarnami pyłu. Pył opadając, nie napotyka żadnych przeszkód ulegał rozproszeniu, a wprowadzony w stanie parowym kwas stearynowy może swobodnie osiadać na jego powierzchni zewnętrznej oraz penetrować w głąb porów, blokując je dla wilgoci. Drugi sposób hydrofobizacji sprowadzał się w uproszczeniu do zmieszania substratów: pyłu wapiennego i domieszki silikonowej - Sarsil® H-15, w parownicy (Vogt i Opaliński, 2009; Vogt i Hołownia, 2010). We wstępnych badaniach określono objętość preparatu, jaką trzeba dodać do pyłu w celu uzyskania optymalnych warunków kontaktu preparatu z ciałem stałym. Otrzymany po modyfikacji materiał był zbrylony w niewielkim stopniu, a jego całkowite rozdrobnienie uzyskano poprzez przecieranie pyłu przez sito o odpowiednim wymiarze oczek. Badanie właściwości tak otrzymanych hydrofobowych materiałów przeprowadzono w oparciu o PN (Polska Norma, 1994), jak również w oparciu o standardowe metody badania materiałów proszkowych z użyciem aparatu Powder Characteristic Tester (Index tables, Tablets & Capsules, 2005) (Tablica 2,3). Oceny stopnia hydrofobizacji materiałów po modyfikacji dokonano, w przypadku proszku hydrofobizowanego parami kwasu stearynowego, w oparciu o procedurę opisaną w Polskiej Normie (1994), oznaczając procentową zawartość kwasu stearynowego. Otrzymany podczas badań pył hydrofobizowany kwasem stearynowym zawierał 0,18% modyfikatora, co jest ilością dopuszczalną przez Polską Normę (1994).W celu oceny właściwości hydrofobowych materiału modyfikowanego roztworem silikonowym do badań zaadaptowano technikę pomiaru zwilżalności ziaren węglowych „film flotation” (Fuerstenau i Williams, 1987) przyjmując, jako materiał odniesienia hydrofobizowaną mączkę wapienną z Kopalni Kamienia Wapiennego w Małogoszczy. Opracowano metodę wyznaczania współczynnika C określonego, jako stopień hydrofobizacji (Vogt i Opaliński, 2009). Średnia wartość C = 84% wskazuje, że materiał modyfikowany preparatem silikonowym uzyskał odpowiednie właściwości hydrofobowe. Tym samym oba materiały po modyfikacji uzyskały zadowalające właściwości wodoodporne. Ponadto, dla badanych pyłów wyznaczono izotermy adsorpcji pary wodnej (Rys. 1). Uzyskane niższe wartości adsorpcji dla materiałów po modyfikacji niż dla proszku surowego potwierdzają, że materiały posiadają charakter hydrofobowy, co pozwala stwierdzić, że obie proponowane metody hydrofobizacji są użyteczne do produkcji wodoodpornego pyłu wapiennego. Analizę termiczną pyłów wapiennych wykonano w celu porównania efektu cieplnego przemian zachodzących podczas ogrzewania pyłów modyfikowanych z efektem cieplnym zachodzącym podczas ogrzewania surowego pyłu wapiennego. W trakcie badań użyto termowagę firmy TA Instruments 2960 SDT ze sprzężonym spektrometrem masowym firmy Balzers TermoStar 300. Otrzymane wynikiprzedstawiono na Rys. 2. Linie ciągłe na Rys. 2a i 2b przedstawiają przebieg krzywych TG, DTG oraz DTA dla pyłu surowego. Linie przerywane zostały otrzymane dla pyłu modyfikowanego kwasem stearynowym (Rys. 2a) oraz preparatem SARSIL® H-15 (Rys. 2b). Na Rys. 3 zobrazowano wyniki analizy zawartości tlenku węgla IV w składzie gazów otrzymywanych podczas rozkładu termicznego pyłu wapiennego (EGA). Krzywa otrzymana dla pyłu modyfikowanego kwasem stearynowym w zasadzie pokrywa się z krzywą otrzymaną dla pyłu surowego. Parametry uzyskane z użyciem aparatu Powder Characteristics Tester umożliwiły scharakteryzowanie pyłów wapiennych nie tylko pod kątem ich właściwości hydrofobowych, ale także właściwości kohezyjnych i przepływowych.
14
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
W pracy przedstawiono wyniki oceny różnych handlowych domieszek (kwas stearynowy, silikony i bitumy) stosowanych w celu hydrofobizacji mączek wapiennych. W oparciu o uzyskane wyniki można stwierdzić, że wszystkie zmieniają właściwości powierzchniowe proszków wapiennych nadając im hydrofobowość. Ta właściwość zależy jednak w poważnym stopniu nie tylko od stosowanej domieszki, lecz także od metody i warunków jej zastosowania.
EN
In the work the evaluation of the usability of commercial agents (stearic acid, silicone preparation and bituminous preparation) for hydrophobization of limestone flours was made. The hydrophobicity of modified materiais was determined and it was stated that all of the used admixtures change the properties of the limestone powder surface causing the water-repellent behavior. However, not only the type of agent but also the method and conditions of its application highly influence the hydrophobicity of treated flour.
15
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Eksploatacja wapieni karbońskich w Czatkowicach trwa od ponad 60 lat. Stanowi ona przykład selektywnego rozwiązania i optymalnego wykorzystania surowcowego niemal każdej występującej w złożu odmiany kopaliny. Sytuacja ta i gromadzone w ciągu kilku dziesiątków lat doświadczenie pozwoliły na kompleksowe użytkowanie wszystkich występujących w złożu odmian kopalin oraz realizowanie optymalnej gospodarki surowcowej stanowiącej wypadkową pomiędzy specyfiką surowcową kopalin z jednej strony, a podążeniem za wymogami rynku zbytu z drugiej. W efekcie tego Kopalnia pozostaje przedsiębiorstwem atrakcyjnym surowcowo. To z kolei posiada pozytywne przełożenie na jej sytuację finansową.
EN
The Carboniferous limestones have been quarried in Czatkowice for more than 60 years. Their winning represents an example of a selective and optimum utilization of almost every rock variety occurring within the deposit. Such a policy and the experience gathered for several tens of years have allowed: introducing complex utilization of all limestone varieties present; - implementing optimum management of the deposit, which results from technological properties of the rocks quarried on one hand and the market requirements on the other. Due to that, the Czatkowice quarry is a mining venture providing sought for, attractive rock products. Their marketing secures the solid financial position of the company.
17
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
W pracy porównano wyniki badań wpływu popiołów lotnych i mączki wapiennej w cemencie na właściwości mieszanki samozagęszczającej się i stwardniałego betonu. Wykazano, że samozagęszczające się mieszanki betonowe zawierające mączkę wapienną jako wypełniacz wykazują mniejszy stopień upłynnienia oraz zawierają większą zawartość powietrza niż mieszanki z dodatkiem popiołów lotnych. Betony samozagęszczające się z dodatkiem mączki wapiennej charakteryzują się większą wodoprzepuszczalnością i wykazują mniejszą odporność na działanie mrozu i środków odladzających w porównaniu do betonów zawierających popioły lotne. Stwierdzono, że wzrost stopnia rozdrobnienia mączki wapiennej wpływa na poprawę właściwości reologicznych mieszanki i stwardniałego betonu. Na podstawie przeprowadzonych badań mikrostruktury próbek betonów wykazano, że mniejsza odporność betonów samozagęszczających się, które zawierają jako wypełniacz mączkę wapienną na działanie mrozu i soli rozmrażającej jest związana ze zwiększonym udziałem porów kapilarnych oraz występowaniem dużych kryształów hydratów w mikrostrukturze tych betonów zawierających mączkę wapienną.
EN
The effect of fly ash and limestone powder in concrete on the properties of self compacting concrete mixture and hardened concrete was studied. It has been found that the self compacting concrete mixtures with limestone flour used as a filler show lower fluidity and higher air content as compared to those with fly ash. The concretes with limestone filler reveal higher water permeability and lower freeze-thaw resistance as well as the resistance to the attack of de-icers as compared to the concretes with fly ash. The rheological properties of the mixture and hardened material are improved at higher fineness of this additive. From the observations of concrete samples microstructure one can conclude that the lower resistance of self compacting concrete with limestone filler is the consequence of the higher capillary porosity and the presence of large crystals of the hydrates.
Proces odgazowania odpadów zawierających części palne jest uzależniony od własności fizykochemicznych odpadów oraz warunków prowadzenia procesu odgazowania. tj. czasu, temperatury i atmosfery gazowej. Obecność innych składników procesowych w mieszaninie odpadów z kalcynatem może także oddziaływać na intensywność procesu oraz skład produktów rozkładu. W artykule przedstawiono wyniki badań nad oddziaływaniem aktywnego tlenku wapnia na szybkość procesu odgazowania oraz skład produktów rozkładu termicznego.
EN
Devolatilisation of waste containing combustible matter depends on physical and chemical properties of waste material and conditions under which the process is carried out i.e. time, temperature and gas atmosphere composition. Presence of other components in waste-limestone powder blend may also influence the process intensity and composition of devolatilisation products. The paper presents the research results of influence of calcium oxide on devolatilisation rate and its composition.
The work proposes a new method of hydrophobization of limestone powder from stearic acid vapour or stearic acid ether solution. The obtained product is characterised by all properties typical of water-resistant materials. The evaluation of these properties has been carried out according to Polish Standard PN-G-11020 and analysed with research methods originally used for powder technique.
20
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
This article outlines an experimental study on different properties such as compressive strength, tensile strength; modulus of elasticity and shrinkage of SCC (Self-Compacting Concrete) containing milled limestone powder. The results show that shrinkage in SCC is approximately twice more than that of normal concrete, while elastic modulus, compressive and tensile strength do not differ significantly.